Frit-Happens !

Lampwork => Borosilicate => Topic started by: Kalorlo on August 20, 2013, 02:20:38 PM

Title: Jellyfish and other boro
Post by: Kalorlo on August 20, 2013, 02:20:38 PM
I've put these up elsewhere, but I think I have enough now to start a thread...

I got out my boro  ;D

I've been joining in Mary K's jellyfish thread on LE (http://www.lampworketc.com/forums/showthread.php?t=243718) that has lots of different techniques for making them. These are gradually getting better!

(Minor, one increasingly wimpy oxycon that I really ought to check the tubing on, but it still *goes* y'know? Taking it to bits would use up my torch time...)

The first one was too big to do anything with in a reasonable time - I scaled down after that. Here they are in order.

(http://farm6.staticflickr.com/5481/9456826057_4363f9e040_m.jpg) (http://www.flickr.com/photos/kalorlo/9456826057/) (http://farm8.staticflickr.com/7427/9462973421_e09cc504fe_m.jpg) (http://www.flickr.com/photos/kalorlo/9462973421/) (http://farm3.staticflickr.com/2888/9479530645_4ce5c3e44c_m.jpg) (http://www.flickr.com/photos/kalorlo/9479530645/) (http://farm3.staticflickr.com/2828/9483415783_d8ab308ee2_m.jpg) (http://www.flickr.com/photos/kalorlo/9483415783/) (http://farm8.staticflickr.com/7323/9486214150_23505602e6_m.jpg) (http://www.flickr.com/photos/kalorlo/9486214150/) (http://farm6.staticflickr.com/5471/9505210156_5aa325fdb7_m.jpg) (http://www.flickr.com/photos/kalorlo/9505210156/)

Jelly 5 with the greenish background gets worn  ;D I am working on my tentacles.

Fizzy fuzzy marble. This is its good angle.

(http://farm4.staticflickr.com/3699/9505210392_b137719079_m.jpg) (http://www.flickr.com/photos/kalorlo/9505210392/) (http://farm6.staticflickr.com/5443/9502412539_afa6ff2ef0_m.jpg) (http://www.flickr.com/photos/kalorlo/9502412539/)
Title: Re: Jellyfish and other boro
Post by: Essex Girl on August 20, 2013, 02:24:54 PM
Those are stunning!
Title: Re: Jellyfish and other boro
Post by: garishglobes on August 20, 2013, 02:44:07 PM
Looks like you've had fun!  :)  I've been keeping half an eye on that thread - it's fun seeing how things are progressing and I like that she's moved on to floral compressions  :)

I love clear backgrounds for jellyfish but I have to say that I'm also a big fan of the sea-like colours of the frit backings and I really like the caramel-coloured one with the green background
Title: Re: Jellyfish and other boro
Post by: Kalorlo on August 20, 2013, 03:04:49 PM
Thank you! Yes, I like the coloured backgrounds for pendants. Even if they add a significant amount of working time at the moment. I think the fritty one needed something else in the gaps because the dots are rather distracting as it is.
Title: Re: Jellyfish and other boro
Post by: chipperpottery on August 20, 2013, 03:19:11 PM
stunning.
Title: Re: Jellyfish and other boro
Post by: Steampunkglass on August 20, 2013, 04:52:21 PM
Lovely jellyfish! I've not looked at LE for ages, interesting as I've never tried the implosion way of making them (yet!)
Title: Re: Jellyfish and other boro
Post by: Dragonfire Glass on August 20, 2013, 06:01:20 PM
They are great Heather :D
Title: Re: Jellyfish and other boro
Post by: Nick on August 20, 2013, 08:20:30 PM
fantastic
Title: Re: Jellyfish and other boro
Post by: Kalorlo on August 21, 2013, 10:11:21 AM
Jelly 7, from Sunday. The jellyfish itself is GA Dragon's Eye. I had no idea what colour the Dragon's Eye was going to come out - could have done a more contrasting background, though I quite like this one. The bright streaks across it are because there are slight gaps between the lines of twistie on the back.

(http://farm4.staticflickr.com/3692/9559390222_6f7ccb3b3e_n.jpg) (http://www.flickr.com/photos/kalorlo/9559390222/) (http://farm3.staticflickr.com/2872/9559390396_9351ba45c8_n.jpg) (http://www.flickr.com/photos/kalorlo/9559390396/)
Title: Re: Jellyfish and other boro
Post by: liquidglass on August 21, 2013, 10:15:03 AM
Lovely work, I particularly like Jelly 7, the  colours are really gorgeous.
Kevin
Title: Re: Jellyfish and other boro
Post by: Barnacle Bay on August 21, 2013, 11:17:50 AM
Love them all esp Jelly 7 too
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on August 22, 2013, 07:33:12 AM
I love Jelly 6 from the top setand of course Jelly 7 is gorgeous. I think the bright streaks because of gaps add to the overall beauty.
Title: Re: Jellyfish and other boro
Post by: Margram on August 22, 2013, 06:06:41 PM
They are wonderful! :)
Title: Re: Jellyfish and other boro
Post by: Kalorlo on August 29, 2013, 09:50:21 AM
Jelly v8: this is persimmon strike over the NS garnet that Sue sent me. I made an encased cane which works for the cap, but after applying the tentacle dots I realised that they were small enough that they'd just be using the outside of the cane, so I added little garnet dots over them and poked them down with my pick. It came out rather darker than I expected, but I think that's my fault for forgetting to change my strike segment back down after the dragon's eye...

The background is a twistie of clear encased in cobalt with blue exotic stripes.

(http://farm6.staticflickr.com/5475/9618835458_88102d9694_n.jpg) (http://www.flickr.com/photos/kalorlo/9618835458/)
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on August 30, 2013, 08:15:10 AM
Another gorgeous pendant.
Title: Re: Jellyfish and other boro
Post by: Kalorlo on September 12, 2013, 10:58:32 AM
These two I used my new thinner pointier tungsten poke, but the main difference was in the amount of stretching I did to the tentacles afterwards: they were looking more or less the same as my previous one before I did that.

Jelly 9: this was NS light ruby with GA persimmon strike on top. This came out the same colour as the persimmon strike on its own, but stopped the tentacles washing out, which is handy. Backed with cobalt.

(http://farm6.staticflickr.com/5346/9725394023_4fa4da74d2_n.jpg) (http://www.flickr.com/photos/kalorlo/9725394023/)

Jelly 10: cap is NS blue caramel - went beige and the beige was not budging! Tentacles are double amber purple. The pendant shape isn't as good because it fell off the punty and landed in my lap when I was shaping the bail and got singed bits of leather apron on it, so I had to pull some of the glass back off. I hadn't added a backing either as it takes me quite a long time to melt those in. The second pic shows the blue fumey part under the cap.

(http://farm8.staticflickr.com/7443/9725394199_43d8751252_n.jpg) (http://www.flickr.com/photos/kalorlo/9725394199/) (http://farm4.staticflickr.com/3727/9728624030_09c9ca76d7_n.jpg) (http://www.flickr.com/photos/kalorlo/9728624030/)
Title: Re: Jellyfish and other boro
Post by: Skyblue on September 12, 2013, 01:40:22 PM
This is a really interesting thread ,I love the jellyfish pendants :)
Title: Re: Jellyfish and other boro
Post by: Kalorlo on September 26, 2013, 09:46:58 AM
Jelly 11.

I've started with my Momka sample pack. This jelly is violet medley - the cap struck but the tentacles didn't. The backing is cloud, which is really pretty and also hard to photograph! The in-hand photo is most representative of looking at it head-on. Turning it about gets light peaches and blue-greens depending.

(http://farm4.staticflickr.com/3770/9941620875_ccf2e70083_n.jpg) (http://www.flickr.com/photos/kalorlo/9941620875/) (http://farm3.staticflickr.com/2889/9941751043_bf3331d667_n.jpg) (http://www.flickr.com/photos/kalorlo/9941751043/) (http://farm8.staticflickr.com/7301/9941622635_b50f727182_n.jpg) (http://www.flickr.com/photos/kalorlo/9941622635/)
Title: Re: Jellyfish and other boro
Post by: JaySpangles on September 26, 2013, 01:45:23 PM
Lovely jellies, such patience.
Title: Re: Jellyfish and other boro
Post by: liquidglass on September 27, 2013, 12:29:03 PM
Best yet Heather, I'm biased of course.  :D

Seriously they are all brilliant ;D ;D
Title: Re: Jellyfish and other boro
Post by: Steampunkglass on September 27, 2013, 04:34:50 PM
ooo yes, I agree, that is the best yet!!!  ;D
Title: Re: Jellyfish and other boro
Post by: Kalorlo on September 27, 2013, 07:06:34 PM
Thank you! New big oxycon = easier shaping  ;D
Title: Re: Jellyfish and other boro
Post by: kerensky on September 27, 2013, 07:42:56 PM
Wow - loving Jelly 11 - really beautiful.
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on September 28, 2013, 08:09:34 AM
Beautiful Heather. Have you tried adding a backing colour to make the tentacles stand out more? I'm thinking of course of an eventual simple diorama, not that I could achieve anything like that  ;)  ;)  ;)
Title: Re: Jellyfish and other boro
Post by: Kalorlo on September 28, 2013, 11:58:26 AM
All the ones that aren't clear have a backing colour. Right now I don't have much idea of what any of the colours will come out looking like (apart from cobalt), so contrast between the tentacles and the backing is somewhat random!
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 02, 2013, 01:58:59 PM
Here are jellies from the weekend.

12. Jellyfish is Momka Alaska Night, backing is Winter Sky. I love how this one came out! The Alaska Night has gone darker at the ends of the tentacles, where they are reheated to pull and twist them out, and is a great blue on the cap. Winter Sky is very well named, it's a chilly frosty blue. My sample was also very bubbly, but in this case that didn't matter, as the tiny trapped bubbles just add sparkle to the background.

(http://farm3.staticflickr.com/2883/10044620285_f0f2f018cc_n.jpg) (http://www.flickr.com/photos/kalorlo/10044620285/) (http://farm8.staticflickr.com/7298/10044717643_c73fb16791_n.jpg) (http://www.flickr.com/photos/kalorlo/10044717643/)

13. Jellyfish is Momka purple thunder, backing is crystal blue. This one got pulled out a bit too much and had to be recondensed, so is all a bit squished. It should have had a larger cap. There's some purple in the cap, while the tentacles are that silver glass caramelly beige colour with hints of pink here and there. The crystal blue is a very pale blue, but still has enough presence not to look like clear. It was also a bit bubbly and I've got some silvery schmutz on the back - overheated or reduced. Again, in this application that doesn't matter so much as it adds some sparkle when viewed from the front.

(None of the colours changed in the kiln).

(http://farm8.staticflickr.com/7391/10044639196_edd5151833_n.jpg) (http://www.flickr.com/photos/kalorlo/10044639196/) (http://farm6.staticflickr.com/5515/10044580184_01e7dac903_n.jpg) (http://www.flickr.com/photos/kalorlo/10044580184/) (http://farm8.staticflickr.com/7355/10044621445_131572bbdb_n.jpg) (http://www.flickr.com/photos/kalorlo/10044621445/)
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on October 03, 2013, 07:01:21 AM
These just keep getting better and better.
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 09, 2013, 11:21:18 AM
Kevin of http://www.meltinglass.co.uk very kindly sent me some Chinese white to try out - I love it! No bubbling whatsoever and it stayed nice and dense even when very thin. Easy to pull good long stringers too.

Jelly 14 has Chinese white tentacles, and I had a go at Mary's little twistie wrap under the cap (cap should probably have been bigger, though - I wasn't sure how far down it would cover them). The cap is Momka almond nugget - really like the way it came out.

(http://farm6.staticflickr.com/5327/10162875413_e0a7d502b9_n.jpg) (http://www.flickr.com/photos/kalorlo/10162875413/) (http://farm3.staticflickr.com/2816/10162876613_466165bfba_n.jpg) (http://www.flickr.com/photos/kalorlo/10162876613/) (http://farm6.staticflickr.com/5514/10162820076_d3d0f6df3e_n.jpg) (http://www.flickr.com/photos/kalorlo/10162820076/)

Jelly 15. I found an incompatibility here: the little tentacles are Chinese white dots poked down into Momka lustrous blue dots, and they have checked. (I'm sure that'll get old fast, but right now it is *fascinating* to see such tiny localised cracking! Don't get that in soft glass). I did search to see whether there was anything about lustrous blue not being suitable for implosions but didn't find it, so am assuming it is the white's fault. The longer tentacles are the other way around and seem to be fine - the blue only really shows through at the ends, though. I forgot which dot colour would end up inside the other - I had meant them to be like the little tentacles until I realised I'd done them the wrong way round. Just as well, really!

The cap was Momka silver iris on top with a wrap of Caribbean coral around the bottom. The silver iris was bubbly and stayed very transparent - don't think this was the best way of using it!

The backing is Momka green envy, which looks greener if you look at the back, but bluer when you look at it through the clear. I like it, it's a very good watery colour.

(http://farm6.staticflickr.com/5513/10162749475_1974178f70_n.jpg) (http://www.flickr.com/photos/kalorlo/10162749475/) (http://farm6.staticflickr.com/5333/10162638384_3e6c69fbe0_n.jpg) (http://www.flickr.com/photos/kalorlo/10162638384/) (http://farm8.staticflickr.com/7347/10162750835_e19c750534_n.jpg) (http://www.flickr.com/photos/kalorlo/10162750835/)

These are tiny mushroom-style jellies with tentacle cane that has layers of Chinese white and Alaska night. The Alaska night shows up better in the front one, where it has gone near black. Caps are Caribbean coral.

(http://farm3.staticflickr.com/2877/10162880303_b942ca0026_n.jpg) (http://www.flickr.com/photos/kalorlo/10162880303/)

(This lot have only been through a soft glass annealing cycle thus far. I don't think I'll bother annealing the cracked one in case it gets worse, but will post again if any of the others strike differently).
Title: Re: Jellyfish and other boro
Post by: Yellow friend on October 09, 2013, 02:46:28 PM
Gorgeous work Heather & lovely colours. The boro glass really lends itself to this subject matter & when the financial fairy smiles again I think I might give it a go. My daughter sent me a pendant from Hawaii that looks a lot like your jelly 10 but has a dark background - I love it :)

Shelia
Title: Re: Jellyfish and other boro
Post by: Marcel on October 10, 2013, 09:27:59 PM
 ;) love the jellies
Title: Re: Jellyfish and other boro
Post by: liquidglass on October 11, 2013, 12:05:05 PM
Heather, I just can't believe how well you have done with that White, it is just amazing. I love all the Jellies but Number 15 has my vote, everything about it. It looks like your holding a bottle of liquid with the jellyfish moving around in it, fascinating.
   
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 17, 2013, 01:16:36 PM
Jelly 16. Momka stormy weather for the cap and small tentacles, Chinese white for the long ones. Backed in lustrous blue, which has a nice pearly look like this and behaves on the surface. I stretched this one out a bit too much, I think, and added the second tentacles too late, so the inner ones nearly terminate partway up. I think maybe I should intersperse the white tentacles with other ones, because the two look too separate.

I really like the stormy weather for caps - I flame struck it just enough so it went dark on all these before adding the clear.

(http://farm8.staticflickr.com/7412/10316902665_beb812ab44_n.jpg) (http://www.flickr.com/photos/kalorlo/10316902665/) (http://farm3.staticflickr.com/2887/10316884554_0f5b26e285_n.jpg) (http://www.flickr.com/photos/kalorlo/10316884554/)

A pair of mushroom-style jellies. I'm not getting these the shape I want them yet. I've done better caps before, but can't quite remember what the difference was in how I did it. I'm trying to do a matching pair for earrings, but can't make two the same size! So mainly I am showing these for the colour of the stormy weather in the caps.

(http://farm3.staticflickr.com/2813/10317070523_d4cc964b66_n.jpg) (http://www.flickr.com/photos/kalorlo/10317070523/)
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on October 17, 2013, 06:42:05 PM
Jelly 16 is wonderful Heather.
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 22, 2013, 02:05:05 PM
I had a go at a Halloween jellyfish, but my tentacles thinned out. This is Momka sunset orange, black rose, with pistachio (M) backing. (Does the M signify anything, by the way?) The orange works great in the cap, not so much in the small dots and the black rose is very transparent. So I guess for the next try I need something to poke inside those dots to make them more opaque. I've also got lemon yellow, sunshine yellow and pumpkin - maybe pumpkin would help? Or a red. Rust is a similar kind of shade, but I don't want them to go pink. I have obsidian as well, to maybe try with the black.

For the backing I'd tried using the black rose to make seaweed shapes before putting on the pistachio - didn't work so well, and the front lens makes some of it not visible. I might try again with very fine white stringer instead, and push it in from behind with a razor to give it some dimension.

(http://farm6.staticflickr.com/5550/10411795845_ac892872e6_n.jpg) (http://www.flickr.com/photos/kalorlo/10411795845/) (http://farm4.staticflickr.com/3671/10411796285_e9c403eecb_n.jpg) (http://www.flickr.com/photos/kalorlo/10411796285/)
Title: Re: Jellyfish and other boro
Post by: liquidglass on October 22, 2013, 02:26:46 PM
Very aquatic looking Heather.
The Pistachio backing works really well. Your Sunset orange looks brilliant, (mine has never come out that dark). Love the idea of seaweed at the back.
I'm in the office and my mate Kip says "best yet, if these are for Halloween  what are you going to do for Christmas"

Kev
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 22, 2013, 02:44:48 PM
LOL! Christmas would have the problem of encasable greens  :P
Hmm, unless I just did red and white... There's silver pine or the sparkly green for backing...
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 29, 2013, 01:10:31 PM
Halloween jelly take 2. I used a whole load of things in the tentacles this time. I used obsidian as the black, which works much better. You can see it is blue-based, but it implodes well enough in tiny dots. I put Momka pumpkin right next to the sunset orange to make larger dots. The pumpkin has pretty much the same saturation as the sunset orange (but yellower), so on its own it is just as thin. I used NS caramel too - that's what is giving the light blue ghostly envelopes. You can see a couple of tentacles are orange and yellow with transparent brownish tips: for those I'd poked a dot of caramel inside them, so was right about the reaction. It works with the colours here, though.

The cap is sunset orange again, with a thin wrap of obsidian and some pumpkin dots around the rim.

For the backing, I used obsidian and did push it in with a razor. It does give it more dimensionality, though on the whole I think it would have looked better if the tentacles were oranger, as they'd have stood out more in front of it. The backing green is Momka guacamole this time. It's more of a lime green than the pistachio (it's also quite bubbly).

(http://farm4.staticflickr.com/3682/10519155916_bfac258ddc_n.jpg) (http://www.flickr.com/photos/kalorlo/10519155916/) (http://farm4.staticflickr.com/3828/10519156676_cdf5af7f10_n.jpg) (http://www.flickr.com/photos/kalorlo/10519156676/)
Title: Re: Jellyfish and other boro
Post by: liquidglass on October 29, 2013, 01:22:22 PM
Oh Heather, they just get better and better, tentacles look brilliant and I still love that orange cap. All the colours work really well together.
Not sure if I prefer the Pistachio or the Pumpkin for the backing, they both suit.



Title: Re: Jellyfish and other boro
Post by: garishglobes on October 29, 2013, 06:45:57 PM
Looking good  :)

You could use Northstar exp. green 5 over white as an encasable green. It comes out nice and strong.... and if you're looking to beef up the opaque red/orange dots, layer a transparent red over the opaque and pull to a stringer, maybe? 
Title: Re: Jellyfish and other boro
Post by: Kalorlo on October 29, 2013, 06:57:49 PM
I'm still going through my Momka sampler before I buy any more colours! But yes, I hear people like the exp. green  ;)

Stringer doesn't work so well for these because the dots are so tiny, you just get the encasing colour mostly. At least with the diameter of stringer I use. So I have been poking one dot inside the other. I'd been thinking about things to put inside the orange, but a transparent red on the outside might be worth trying, ta.
Title: Re: Jellyfish and other boro
Post by: sea-thistle on October 30, 2013, 02:26:00 AM
I love all of them, very beautiful!!
Title: Re: Jellyfish and other boro
Post by: Kalorlo on November 28, 2013, 01:18:33 PM
Boro jelly 19, had a bad day all round here, with colour choice and shaping... The jellyfish is Momka exotic citrus and Chinese white - I was surprised it went so pink! Was expecting more yellows. There is more white in the background, so I shouldn't have put it in the tentacles too. The backing colour is the part I do like, it is Momka green flambé and has all sorts of colours in it. I've taken a shot of the back just to show how different it looks on the surface vs encased. I like! ('Scuse the bubbly scum).

(http://farm8.staticflickr.com/7408/11092980636_eb2e016435_n.jpg) (http://www.flickr.com/photos/kalorlo/11092980636/) (http://farm4.staticflickr.com/3815/11093003004_d209f2c881_n.jpg) (http://www.flickr.com/photos/kalorlo/11093003004/) (http://farm3.staticflickr.com/2854/11093003444_4b4c9b0d68_n.jpg) (http://www.flickr.com/photos/kalorlo/11093003444/)

Jelly 20, much better! Here the jellyfish is Momka silver flambé and the backing is American Beauty. The silver flambé seems a fairly similar kind of thing to the green - it has all sorts of muted colours in it.

(http://farm3.staticflickr.com/2889/11093114983_40523a35b4_n.jpg) (http://www.flickr.com/photos/kalorlo/11093114983/) (http://farm3.staticflickr.com/2877/11092990766_06ec93e989_n.jpg) (http://www.flickr.com/photos/kalorlo/11092990766/)

Jelly 21. The jellyfish is Momka silver pine. I couldn't find anything about whether you could implode this colour, it being a green. I did find reference to encasing it ok, so decided to try and see. I have what appears to be a small amount of checking in the cental tentacles, so it looks like the answer is no. The cap is fine, so picking another tentacle colour to go with it should work. It's a pretty blue-tinged green - no problem keeping this for myself! The backing was the silver flambé, which changes colour quite a bit depending on the angle of the light. Unencased on the back it looks similar to the green flambé, with loads of reddish purple. Straight on in normal light you mostly see greens and blues with a little purple, and in very bright direct light some more purple is visible.

(http://farm3.staticflickr.com/2864/11093013414_eca156973d_n.jpg) (http://www.flickr.com/photos/kalorlo/11093013414/) (http://farm8.staticflickr.com/7293/11092991956_9e45612b6c_n.jpg) (http://www.flickr.com/photos/kalorlo/11092991956/)
Title: Re: Jellyfish and other boro
Post by: Steampunkglass on November 28, 2013, 02:25:33 PM
Loving the jellyfish, some great colour effects there!  ;D  ;D ;D
QuoteBut yes, I hear people like the exp. green   ;)
Oooohhh yes, although first few times when I first tried using it stubbornly wanted to stay blue, then when I tried to use it as a nice blue colour it striked to a lovely green  ::) ::) ::) I've used it for jellyfish and makes a nice cap on it's own. I'd think as it's not a very deep encasement you could probably get away with most opaque greens, I've had the odd one cause cracking or tiny bubbles but that's only if I've used a lot deep inside a marble. I use forest green for leaves on flower marbles and that seems (mostly) fine although sometimes it can leave a few extra tiny bubbles. I've heard that a rather well know marble maker uses a thin layer of yellow over blue or black to make canes of green in his implosions.....
Title: Re: Jellyfish and other boro
Post by: Lotti on November 28, 2013, 06:05:45 PM
I really like 20 and 21, have had a go but my attempts were rubbish, must have another go!  I love exp green, have a lovely mushroom made with it and a marble with a couple of 'inside' swirls (not a great marble, but loved the colours). :)
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on November 28, 2013, 08:32:17 PM
They just keep getting better and better Heather.
Title: Re: Jellyfish and other boro
Post by: liquidglass on December 02, 2013, 04:01:53 PM
I love the colour choices, esp 20 and 21. The green flambe on the back of 19 is fantastic.  :) :)
Title: Re: Jellyfish and other boro
Post by: Kalorlo on December 04, 2013, 10:28:21 AM
I made some Christmas jellyfish  ;D

Jelly 22. This is Chinese white, Momka carmen red, and the backing is Momka sparkly green. I like the carmen red over white on the cap, but on its own in the tentacles it thins out too much. That's why there's such a gap between the upper and lower tentacles: the outer ones were all red and they don't show up enough. The sparkly green's transparent and not a super-saturated one - used like this, the sparkle I got looks more like airy glass. Not bad, just not blingy.

(http://farm4.staticflickr.com/3729/11196359004_46b0881c19_n.jpg) (http://www.flickr.com/photos/kalorlo/11196359004/) (http://farm6.staticflickr.com/5506/11196339535_cb01725144_n.jpg) (http://www.flickr.com/photos/kalorlo/11196339535/)

Jelly 23. I made cane with Chinese white encased in Momka cherry brandy for this. The tentacles are a mixture of that and pure white ones. I think the cane worked well. It's a pinker red than the carmen, though. The backing for this is Momka ivy green, which is an absolutely gorgeous colour, reasonably opaque.

(http://farm4.staticflickr.com/3791/11196479413_2d4635960f_n.jpg) (http://www.flickr.com/photos/kalorlo/11196479413/) (http://farm8.staticflickr.com/7292/11196368786_bb99ca3147_n.jpg) (http://www.flickr.com/photos/kalorlo/11196368786/)

Here they are side-by-side.

(http://farm4.staticflickr.com/3815/11196341215_f453974620_n.jpg) (http://www.flickr.com/photos/kalorlo/11196341215/)
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on December 04, 2013, 07:20:03 PM
I love both of them Heather.
Title: Re: Jellyfish and other boro
Post by: Skyblue on December 08, 2013, 07:32:26 AM
Ive just read all the way through this post and the jellyfish are amazing Heather . Its fascinating watching how you are experimenting with the colours and backgrounds etc.. :)
Title: Re: Jellyfish and other boro
Post by: Kalorlo on April 02, 2014, 10:38:53 AM
Jelly 24

I used two Momka striped shorts for this, applying them as twisties. The jellyfish is the blue/beige cane. I used the pink/clear one as the background, then put a stripe of cobalt behind it to make it show up better (had no idea before applying the pink how much was clear and whether any of it would strike). I had to adjust the photo colouring a bit in the top 2 pics - the pink-coral was showing up as bright red, which it really isn't in reality!

(https://farm6.staticflickr.com/5528/13569365884_4fbeb30cfe_n.jpg) (https://flic.kr/p/mF5xJd) (https://farm8.staticflickr.com/7116/13569004555_a094d6bb50_n.jpg) (https://flic.kr/p/mF3Gjp)

Cane
(https://farm8.staticflickr.com/7006/13569058593_69f2d436dc.jpg) (https://flic.kr/p/mF3Yo6)

Anemone
This anemone cab was made with the blue/green Momka short and a small dot of blue exotic on the back.
(https://farm3.staticflickr.com/2813/13569002175_4803203f2f_n.jpg) (https://flic.kr/p/mF3FBn) (https://farm8.staticflickr.com/7345/13569003055_5b95bdbe79_n.jpg) (https://flic.kr/p/mF3FSx)

Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on April 03, 2014, 07:30:23 AM
Beautiful jellyfish as always Heather, but I was more taken with the nail polish display  ;D ;D ;D
Title: Re: Jellyfish and other boro
Post by: liquidglass on April 03, 2014, 08:35:13 AM
Fantastic Heather !! :)
I love using the striped, you can get some really lovely colour combinations


 
Title: Re: Jellyfish and other boro
Post by: Kalorlo on April 03, 2014, 09:32:01 AM
Thank you!

LOL Pat! That's one of the magnetic polishes that do a mica-shift type of thing.  :D
Title: Re: Jellyfish and other boro
Post by: hopejacare on April 03, 2014, 10:34:24 AM
Oh my I can't believe I have not come across this thread before. I absolutely love jellyfish.
I had a wee go making teeny ones on my hot head and just love it. These are stunning.......
Just so beautiful. Cheers Claire Xx
Title: Re: Jellyfish and other boro
Post by: Dragonfire Glass on April 21, 2014, 09:36:10 PM
Heather,they are beautiful  ;D
Title: Re: Jellyfish and other boro
Post by: Kalorlo on August 06, 2014, 01:20:18 PM
Jelly 26 - Sasha's oil slick (not treated right I think, but hey) and Chinese white, with GA peacock frit on the cap and background, backed by Momka beige/brown short. A bit wibbly-shaped because I noticed a surface defect after the first time through the kiln, so removed that next time, but didn't sort the shape - I was just hanging on to it with pliers rather than puntying it up again.

(https://farm6.staticflickr.com/5552/14837435154_104124f55f_n.jpg) (https://flic.kr/p/oB8Jxu) (https://farm4.staticflickr.com/3857/14837435664_7d60cfc049_n.jpg) (https://flic.kr/p/oB8JGh)

Momka short - went pastel and checked when encased, but looks way more interesting on the back surface!

(https://farm4.staticflickr.com/3879/14653250277_2551326074_n.jpg) (https://flic.kr/p/ojRJNa)

Jelly 28 with checks - Momka beige/brown short backed by GA dragon's eye frit. The in-hand pic has the best idea of what the background really looks like most of the time.

(https://farm4.staticflickr.com/3913/14653100800_e9aa363816_n.jpg) (https://flic.kr/p/ojQYmY) (https://farm4.staticflickr.com/3881/14859664843_3f3fcf96eb_n.jpg) (https://flic.kr/p/oD6EDZ) (https://farm6.staticflickr.com/5568/14653251177_8ee1dbf17f_n.jpg) (https://flic.kr/p/ojRK4F)

Jelly 27 - blue exotic and Chinese white, backed with Momka yellow/pearly green cane.

(https://farm6.staticflickr.com/5552/14837436954_0fd20d9ab8_n.jpg) (https://flic.kr/p/oB8K5w) (https://farm4.staticflickr.com/3898/14653157399_c0d6f568ca_n.jpg) (https://flic.kr/p/ojRgbP) (https://farm4.staticflickr.com/3881/14837437374_455376160f_n.jpg) (https://flic.kr/p/oB8KcL)

Obtainium gremlin - my first gremlin in boro. Need to add some colours with more contrast to my eye murrini - you can see the slight lines in very bright light like here, but otherwise it looks more like uniform misty teal. (And use black for the pupil - I just went with cobalt this time). I scummed up the back rather too. I should dilute my *obtainiums for these, I think! Wasn't intending it to be quite so opaque.

(https://farm4.staticflickr.com/3865/14653181308_cd8933c837_n.jpg) (https://flic.kr/p/ojRoi3) (https://farm6.staticflickr.com/5568/14839804475_ca4e9a561b_n.jpg) (https://flic.kr/p/oBkSRR)

Harvest beads - NS silver bullet with GA dragon's eye frit. My first boro beads. I'm not sure I like making beads in boro - getting them into shape is very annoying (these are *not* the roundest...), and pendants are much more fun. They are very pretty, though.

(https://farm6.staticflickr.com/5570/14839442962_9d2b950963_n.jpg) (https://flic.kr/p/oBj2oS) (https://farm4.staticflickr.com/3907/14653182718_ab81233bb2_n.jpg) (https://flic.kr/p/ojRoHm)

Multi BHB - NS multi with GA dragon's eye frit. Swampy.

(https://farm4.staticflickr.com/3924/14859667463_90593c7771_n.jpg) (https://flic.kr/p/oD6Fra) (https://farm6.staticflickr.com/5575/14816830736_3e7c0e1332_n.jpg) (https://flic.kr/p/ozj8yU) (https://farm6.staticflickr.com/5565/14839444312_e637910031_n.jpg) (https://flic.kr/p/oBj2N9)
Title: Re: Jellyfish and other boro
Post by: Rascal on August 06, 2014, 02:27:35 PM
They are lovely, the gremlin is really fun. My favourite is Jelly 27, the 'tenticles' look stunning the way they 'swirl' in the water. 
Title: Re: Jellyfish and other boro
Post by: Kalorlo on August 14, 2014, 01:32:12 PM
Jelly 29 is NS silver seaweed and Chinese white, with dark orange backing.

(https://farm4.staticflickr.com/3903/14724449820_a0592030e4_n.jpg) (https://flic.kr/p/or9DWu)

I made dragon eye murrini and another gremlin (NS rootbeer body, over clear and encased. Silver bullet lips and eyelid, random end-of-pull vine twistie).

(https://farm4.staticflickr.com/3850/14908060101_3fbd75cbe1_n.jpg) (https://flic.kr/p/oHnGSZ) (https://farm4.staticflickr.com/3893/14724566277_fbe27c28ae_n.jpg) (https://flic.kr/p/orafyn) (https://farm4.staticflickr.com/3925/14908061431_397508777f_n.jpg) (https://flic.kr/p/oHnHgV)
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on August 14, 2014, 02:03:29 PM
Beautiful work Heather.
Title: Re: Jellyfish and other boro
Post by: Essex Girl on August 14, 2014, 02:54:58 PM
Love the jellyfish and the gremlin - I am also impressed by the paintwork on your fingernail ;)
Title: Re: Jellyfish and other boro
Post by: Moira HFG on August 14, 2014, 11:51:57 PM
Those jellyfish are wonderful - really inspirational!
Title: Re: Jellyfish and other boro
Post by: Kalorlo on February 06, 2015, 01:23:24 PM
Some more jellyfish.

NS Blue Moon jellyfish with backing of NS silver pearl (the backing colour in hand is more accurate).

(https://farm9.staticflickr.com/8594/16235626800_5bb5b6222d.jpg) (https://flic.kr/p/qJFQd1) (https://farm9.staticflickr.com/8565/16397059866_de7974904a.jpg) (https://flic.kr/p/qYXdCJ)

Blue Moon jellyfish with TAG caramelo backing

(https://farm8.staticflickr.com/7383/16236802179_72db1d3f74.jpg) (https://flic.kr/p/qJMRBa) (https://farm8.staticflickr.com/7346/15800530834_56c9ff6f59.jpg) (https://flic.kr/p/q5eRkq) (https://farm8.staticflickr.com/7297/16423022955_481e2ec660.jpg) (https://flic.kr/p/r2fhyc)

Momka Almond Nugget jellyfish with blue moon backing

(https://farm8.staticflickr.com/7318/15800531564_26a7fa2d45.jpg) (https://flic.kr/p/q5eRy1) (https://farm8.staticflickr.com/7370/16235630770_f0f00e17fa.jpg) (https://flic.kr/p/qJFRos) (https://farm8.staticflickr.com/7436/16235631010_ea90de0c82.jpg) (https://flic.kr/p/qJFRsA)

Momka Silver Flambe jellyfish with blue moon backing

(https://farm8.staticflickr.com/7445/16237136727_3b0172f43d.jpg) (https://flic.kr/p/qJPz4e) (https://farm8.staticflickr.com/7318/15802986233_5b6b753791.jpg) (https://flic.kr/p/q5sreT) (https://farm8.staticflickr.com/7366/16237137247_b90722981c.jpg) (https://flic.kr/p/qJPzdc)
Title: Re: Jellyfish and other boro
Post by: Jennie Lamb on February 06, 2015, 02:54:38 PM
Beautiful Heather....I love the length you get on their 'tails' so different
Title: Re: Jellyfish and other boro
Post by: Pat from Canvey on February 10, 2015, 08:37:43 PM
Lovely work Heather.