Frit-Happens !

Lampwork => Common Problems => Topic started by: emvee on August 17, 2013, 10:25:12 AM

Title: Disks
Post by: emvee on August 17, 2013, 10:25:12 AM
Hi, I'm having problems making disks. I either don't put enough or too much glass on and they always look bumpy?? Any tips would be great . Thanks
Title: Re: Disks
Post by: Kaz on August 17, 2013, 11:32:55 AM
Six years of beadmaking and I still can't make a great disk bead!
Kazx
Title: Re: Disks
Post by: jammie on August 17, 2013, 12:19:55 PM
hmm, Helen's got a really good disc tutorial on etsy!
Title: Re: Disks
Post by: helbels on August 17, 2013, 02:23:37 PM
What type of discs are you making?

With discs there's a VERY fine line between too much glass and not enough.  I think you are probably not getting that line quite right yet.  If the discs are bumpy it's usually because there are areas of the bead that haven't got enough glass in them (so those bits look like little dents), while other areas of the disc are actually just right.  Once you get the amount of glass to "nearly enough", then try just adding some small dots of glass to the disc, then melting in... so you are only adding a weeny bit more at a time, and see how you get on that way.
Title: Re: Disks
Post by: mizgeorge on August 17, 2013, 04:12:22 PM
I like making discs with commercial stringer - makes it very much easier for me as I'm cack-handed at adding little bits at a time!
Title: Re: Disks
Post by: emvee on August 18, 2013, 08:37:58 AM
Thanks for your replies. I'll try adding dots instead of going all way round. I'm using brass roller to make the shaped disks not the flat type.
Title: Re: Disks
Post by: Kaz on August 30, 2013, 07:42:10 AM
I did make these this weekend - it's a start!

(http://farm4.staticflickr.com/3807/9604889879_0ed45acfe6.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/9604889879/)
IMG_2710 (http://www.flickr.com/photos/cheekycherubdesigns/9604889879/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr

Kazx
Title: Re: Disks
Post by: petrahergarden on August 30, 2013, 12:44:13 PM
I think they look really nice!!
Title: Re: Disks
Post by: Lynnybobs on August 30, 2013, 12:48:24 PM
They remind me of the liquorice Catherine wheel sweets - lovely!
Title: Re: Disks
Post by: helbels on August 30, 2013, 01:46:36 PM
Wow Kaz, they are fabulous, love them (but then again, you never make anything I dislike!)
Title: Re: Disks
Post by: kerensky on August 30, 2013, 03:48:29 PM
Quote from: Lynnybobs on August 30, 2013, 12:48:24 PM
They remind me of the liquorice Catherine wheel sweets - lovely!

Just what I was thinking - l love Liquorice :-)
Title: Re: Disks
Post by: emvee on August 31, 2013, 09:21:18 AM
Kaz those are lovely.