Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: Trudi on July 24, 2013, 03:03:30 PM

Title: Question weather proof Fused glass??
Post by: Trudi on July 24, 2013, 03:03:30 PM
I have a fusing question

If I fuse my glass (to  standard schedules) would it be weather proof – someone has asked me if I can make a house number for them.
My beads have survived outside, but I've never tried it with fused work!

Thanks

Trudi x
Title: Re: Question weather proof Fused glass??
Post by: ♥♥Tan♥♥ on July 24, 2013, 03:25:11 PM
A lot of my fused stuff has been hanging outside for a couple of years now and it is fine the only issue I had was the copper hangers weathered through.
Title: Re: Question weather proof Fused glass??
Post by: Trudi on July 24, 2013, 03:26:08 PM
Cheers Tan

I thought it would be ok   .. I've just never done it!
Title: Re: Question weather proof Fused glass??
Post by: ♥♥Tan♥♥ on July 24, 2013, 04:12:26 PM
All of them went through the frosts with no problem as well
Title: Re: Question weather proof Fused glass??
Post by: MeadMoon on July 24, 2013, 05:06:51 PM
I've seen other peoples' fused glass displayed outside with no problems, but I haven't tried any of mine yet.  They're so small (made in an SC2) that I'd probably lose them in the jungle that I like to call a garden!
Title: Re: Question weather proof Fused glass??
Post by: flame n fuse on July 24, 2013, 10:53:41 PM
we've successfully used house numbers,  - made a mould and filled it with frit, and they've withstood the last 4 Scottish winters (and summers), so I'd say that they'll stand pretty much anything
Title: Re: Question weather proof Fused glass??
Post by: Trudi on July 25, 2013, 05:32:32 PM
Thank you everyone x
Title: Re: Question weather proof Fused glass??
Post by: CrazyKiln on August 16, 2013, 09:29:56 AM
If you use nichrome wire rather than copper you should find that weathers better.
Title: Re: Question weather proof Fused glass??
Post by: Trudi on August 17, 2013, 12:07:38 PM
Thank you