Just wondered if anyone could advise me on whether anti tarnish tabs/strips etc are any good, and if so, which ones you'd recommend please. I know Palmer metals do them but there seem to be lots of different types out there - any help appreciated!
Title: Re: Anti Tarnish products - any good?
Post by: Blue Box Studio on July 21, 2013, 12:07:36 PM
I bought some in from Intercept in the US a couple of years ago and didn't find they helped at all.  After people said they were good, I bought more from Palmers and new made jewellery, straight into a grip seal bag with a Palmers tab, as much air as I can remove is removed and within a couple of months it is all tarnished. They say 1 tab is enough for x square cms, so initially I put several of them inside my fairs stock box with earrings on stands ready to go out - they tarnished between weekly fairs. :( I can't say I'm impressed or would recommend. 

If I'm doing something wrong, sopmeone please tell me, because I'm thinking these plastic squares are up there with the 'Emperor's new clothes'.
Title: Re: Anti Tarnish products - any good?
Post by: SallyR on July 22, 2013, 08:22:03 AM

Thanks for this, Sue - from your experiences, they don't sound too promising.

Anyone else tried them?