Frit-Happens !

Lampwork => COE 104 => Topic started by: mindy23 on November 08, 2007, 11:58:45 AM

Title: Cim Khaki
Post by: mindy23 on November 08, 2007, 11:58:45 AM
Hi everybody,
Can anyone give me some tips on CIM khaki?  I have a kilo I bought a little while back but hadn't got round to using yet.  The rods are really, really shocky to start with and when I have tried to make into a bead it just boils and scums and froths etc etc.  I tried it as a base and the frothy bit crept up round all the other colours.  Can anyone give me any advice on what I could try or does it sound like there may be something amiss with this batch? It looks so nice I'm dying to use it in something. ???
Title: Re: Cim Khaki
Post by: Marijane on November 08, 2007, 01:39:35 PM
By coincidence I have done the same, bought some ages ago and just got it out to play this morning.  Mine is not especially shocky, but it did boil when I got it too hot. I only made a couple of beads as I have been trying out colour combo's today.  It seemed to work okay with frit.  (Not sure about combo's I chose thought - probably won't be posting results!)

Mari 
Title: Re: Cim Khaki
Post by: *rowanberry* on November 08, 2007, 05:31:00 PM
When I was testing it for them I got the same, it devitted on me, and was very shocky and did weird boiling scummy bubbly things. that was back in august.

might be worth getting Kathy Seamonds onto it?
Title: Re: Cim Khaki
Post by: mindy23 on November 09, 2007, 10:06:38 AM
I'll get in touch with Kathy, she's so helpful I didn't want to pester before I had asked about anyone elses experience.  It's such a nice colour I'm dying to use it! 
Title: Re: Cim Khaki
Post by: Chameleon on November 12, 2007, 10:34:26 PM
I havent had any probs with it ? maybe a diff batch mine isnt shocky and i havent managed to boil it either. IT does seem to love silver leaf / foil....goes gold
Title: Re: Cim Khaki
Post by: Vicki on November 12, 2007, 11:30:09 PM
Mine boiled too, I thought it was just me ;D