Post by: KatheL on May 16, 2013, 12:14:53 AM
I need some very saturated white, by some called enamel white I believe. What is best, what is available in Europe?
It is for making japanese style murrini. Actually I believe that last year I read somewhere that Satake had made a 104 coe white especially for that, but I can't find it again, so maybe my memory is playing me a trick.
Kugler should have an enamel white, I have a Kugler white, but it is not very saturated, so I wonder if they have a "normal" white too?

Also, does anyone in Europe sell frits from Glassdiversions.com, I am particularly looking for Coffee Bean?

Kathe, Denmark
Title: Re: looking for very saturated white and coffe bean frit
Post by: Shirley on May 16, 2013, 07:46:47 AM
Kathe, I have just ordered enamel white to stock in my Val Cox shop. It should be here in about 7-10 days. I don't know whether I have anything similar to coffee bean. I'll have a look.

Thanks for your order, too :)
Title: Re: looking for very saturated white and coffe bean frit
Post by: KatheL on May 16, 2013, 08:52:38 AM
Sounds good, but what I am looking for is white rod, coe 104...would like an update if you find some coffee brown!
Kathe
Title: Re: looking for very saturated white and coffe bean frit
Post by: Shirley on May 16, 2013, 08:54:53 AM
The coffee brown looks really nice. Afraid I don't have a brown blend at all, just bitter sweet, which is a dark chocolate.

Manda at Mangobeads has some Kugler rods, so I don't know whether it is worth you asking her?
Title: Re: looking for very saturated white and coffe bean frit
Post by: KatheL on May 16, 2013, 09:05:43 AM
Thanks, will do!
Kathe
Title: Re: looking for very saturated white and coffe bean frit
Post by: Beadbug on May 16, 2013, 03:32:23 PM
Hi Kathe
You could try Vickie at http://www.vickiesemporium.co.uk/frit-addiction-2/ she has lots of 104 frit.
Title: Re: looking for very saturated white and coffe bean frit
Post by: KatheL on May 16, 2013, 04:11:41 PM
Thanks, have been looking, no luck so far.

I think I need to try the special Effetre white, called Smalto, sold by Gunnar Haag in Germany:
http://www.ebay.co.uk/itm/NEU-Smalto-3-4mm-Spezial-EXTRA-DICHTES-WEIs-Effetre-S465H-/370672790697?pt=K%C3%BCnstlerbedarf&hash=item564dd1eca9

Or hope that Kugler glass will make an enamel white in the Beadmaking 104 series.

Has anybody heard of a white coe 104 Satake glass? I stumpled upon it sometime this winter, but didn't save the link, and now I can't find anything about it, not even on Satake's site!

Kathe, Denmark
Title: Re: looking for very saturated white and coffe bean frit
Post by: Dragonfire Glass on May 16, 2013, 05:19:59 PM
Try Debs: debbie@silverartz.co.uk she sells satake glass
Title: Re: looking for very saturated white and coffe bean frit
Post by: June on May 17, 2013, 03:11:53 PM
Quote from: Beadbug on May 16, 2013, 03:32:23 PM
Hi Kathe
You could try Vickie at http://www.vickiesemporium.co.uk/frit-addiction-2/ she has lots of 104 frit.

If you email Vickie she may be able to do a blend for you as I think she is looking to offer a custom blend service  :)
Title: Re: looking for very saturated white and coffe bean frit
Post by: arachnia on May 17, 2013, 06:41:04 PM
Quote from: June on May 17, 2013, 03:11:53 PM
Quote from: Beadbug on May 16, 2013, 03:32:23 PM
Hi Kathe
You could try Vickie at http://www.vickiesemporium.co.uk/frit-addiction-2/ she has lots of 104 frit.

If you email Vickie she may be able to do a blend for you as I think she is looking to offer a custom blend service  :)

Thanks June and Caroline :)


I am offering a custom blends service hopefully will be set up by Monday.
I have effetre white and the darkest brown I have at the moment is dark chocolate brown.
I am waiting on some cutting bits to do any other colours.
Title: Re: looking for very saturated white and coffe bean frit
Post by: KatheL on May 18, 2013, 04:26:36 PM
Hi Vickie,
When you say Effetre white, is it standard white nr. 204, or smalto white nr. 465?

I think there must be a variety of dark browns in the Coffee Bean frit, some of them reactive. If you come up with something similar, please let us know! Meantime I will try blending something myself.
Kathe
Title: Re: looking for very saturated white and coffe bean frit
Post by: arachnia on May 18, 2013, 11:48:44 PM
I will let you know if I find something of that colour :)