Frit-Happens !

Lampwork => Common Problems => Topic started by: Mandy on April 09, 2013, 08:27:35 AM

Title: enameling masks ..
Post by: Mandy on April 09, 2013, 08:27:35 AM
After watching Sally doing her demo on Friday, I rushed a cross flame off and brought some enamel. I can't wait to give them a try while I still remember what to do with them but I'm a little afraid..Could someone point me in right direction on where to get a mask. I was intending just to buy a simple dust mask but after reading a couple of thread I fear this might not be adequate...Thanking you in advance xx
Title: Re: enameling masks ..
Post by: babyshoes on April 09, 2013, 09:30:08 AM
Arco stock pretty much all such safety equipment, in every variable you may require. You could also try RS components - they have a decent selection of safety gear. Even B&Q would probably have something adequate, but I'd expect it to be pricey.
Title: Re: enameling masks ..
Post by: Mandy on April 09, 2013, 10:16:53 AM
Thank you for you help, I did have a nose at the ones tuffnells do but they don't sell them on there own..Off to have a nose x
Title: Re: enameling masks ..
Post by: Zeldazog on April 09, 2013, 10:19:10 AM
If you have a screwfix near to you, they normally sell a range of dust masks to meet different requirements.