Frit-Happens !

Lampwork => Common Problems => Topic started by: Lynnybobs on February 10, 2013, 07:33:49 PM

Title: Beads not shiney ?
Post by: Lynnybobs on February 10, 2013, 07:33:49 PM
Been out in the shedio today having a play but my beads have come out with a dull surface - almost like they have had quick dip in etching fluid - any ideas why this may be ?
I was wondering whether it was due to the cold as the shedio is also quite damp - so I thought perhaps condensation on the glass rods ?
Also it was taking an absolute age to melt the glass but I am on a hot head so again thinking its down to the propane being very cold as its only been hovering just above freezing today.
Title: Re: Beads not shiney ?
Post by: helbels on February 10, 2013, 07:38:15 PM
What colours were you using? Wondering if it could be devit....
Title: Re: Beads not shiney ?
Post by: Lynnybobs on February 10, 2013, 07:41:09 PM
I tried french blue, dark ivory, trans teal, white, trans cobalt blue all effetre - the transparents are more shiney than the opaques but still not as I would have expected ? They haven't been annealed though - maybe that would help bring back the shine?
Title: Re: Beads not shiney ?
Post by: Shirley on February 10, 2013, 07:47:11 PM
Could it be dust from vermiculite, the blanket or bubbles? If you have the beads too hot when they go in they might be picking up something.
Title: Re: Beads not shiney ?
Post by: helbels on February 10, 2013, 07:52:32 PM
When I was on a Hothead, I did sometimes think that the beads looked shinier once annealed, so could be worth a try......