I have seen quite a few inclusions recently that appear as gold once fired - does anyone know if this is likely to be actual gold leaf or is there another metal that appears a gold colour when fired? x
Could be gold leaf, might be silver foil or leaf as some colours of glass will turn it to a gold colour. Could also be silver encased with amber. Have you got any pics?