Only a little one as I only have an SC2.
Would love some tips, as I was a bit disapointed with it.
Should I have slupmed more?
If so how should I change my schedule?
Ths is what I used...

R1 222
L1 685
H1 20m
R2 full
L2 516
H2 60m
R3 83
L3 371
H3 off

(http://i1088.photobucket.com/albums/i325/purple_cobwebs/slumped.jpg)
Title: Re: My first slumped bottle.
Post by: Blue Box Studio on February 03, 2013, 12:02:34 PM
Found this thread http://www.frit-happens.co.uk/forum/index.php?topic=1200.0 - how do the temps compare to what you used?  This is still on my list of things to do in an SC2, so interesting to see how you get on :)
Title: Re: My first slumped bottle.
Post by: Shades of Colour on February 03, 2013, 12:08:20 PM
Hi.  I've just started slumping and for my first piece I used a similiar schedule as yours and it didn't work.  I bought some moulds and the one below came with them and it has been working for me and I'm using a SC2 as well.

rate - 200, Temp - 520, hold 25 mins
rate - 330, Temp - 650, hold 20 mins
rate - full, Temp - 516, hold 50 mins
rate - 60, Temp - 370, hold 0

Hope it helps  :)
Title: Re: My first slumped bottle.
Post by: Purple Cobwebs on February 03, 2013, 04:37:12 PM
Thanks Alison x
Title: Re: My first slumped bottle.
Post by: MeadMoon on February 04, 2013, 10:20:06 AM
This is the schedule that I use for slumping small wine bottles in my SC2.  It's based on a schedule from the Brad Walker book.

Seg.   Rate   Temp   Hold
1        278     593      10
2        139     704       0
3       Full      804      5
4       Full      554     60
5        56       399       0

For slumping fused Bullseye glass into a mould, my schedule is practically the same as Alison's.
Title: Re: My first slumped bottle.
Post by: Purple Cobwebs on February 04, 2013, 11:12:16 AM
Ooh, brilliant, thanks Elaine :)
Title: Re: My first slumped bottle.
Post by: Glyn Burton on February 04, 2013, 07:51:55 PM
Is it just me but I cant see the fascination of slumped bottles, they just look like a flat bottle. I student asked if she could slump some today so we loaded a kiln with 20 of the damn things and all we will get is 20 flat bottles it seems like a waste of kiln time to me. If it floats your boat then fine thats up to you but for the life of me I cant see the attraction.
Title: Re: My first slumped bottle.
Post by: Shades of Colour on February 04, 2013, 08:30:00 PM
I was possibly thinking of doing it with an empty champagin bottle.  The bottle was bought for me as a 40th birthday present last year, obviously the champaign is gone but I liked the bottle and thought it would be a way to keep hold of the present bought for me for a special birthday!!  On closer looking of the bottle I think its only a label anyway so once thats taken off it won't look any different to any other wine/champaign bottle  :(
Title: Re: My first slumped bottle.
Post by: helbels on February 04, 2013, 08:49:32 PM
I think the idea is that you stick the label back on once it's slumped, so you get a slumped bottle with your nice label on it :)
Title: Re: My first slumped bottle.
Post by: flame n fuse on February 04, 2013, 09:13:48 PM
they used to get turned into ash trays before the smoking ban in pubs
Title: Re: My first slumped bottle.
Post by: Rascal on February 04, 2013, 09:52:03 PM
I've seen some lovely ones which are used as dishes/plates to serve things on. For me it's like a lot of art, it's personal taste but even if it's not to my taste I can still admire the skill. Especially when it involves glass and I've started to understand how easily it can misbehave!
Title: Re: My first slumped bottle.
Post by: Pat from Canvey on February 05, 2013, 08:23:51 AM
If you prop up the neck of the bottle, you can get a nice handle if you are going to use the bottle for snacks. I'll see if I can post a picture later.

I've managed the picture now, partially slumped with the bottom weighted for balance.
(http://pic20.picturetrail.com/VOL1426/5604171/22750186/405530190.jpg)
Title: Re: My first slumped bottle.
Post by: MeadMoon on February 05, 2013, 10:26:25 AM
Oh, I really like that one Pat.