I am very new to fusing but have managed to fuse together some sheets of glass with frit and/or millefiori chips and then slump the fused sheets into small dish moulds. I understand that fully fused glass wants to be about 6mm - i'm finding this a bit too thick for the size of dish i'm making. Is there a way of fully fusing decorative elements into a glass sheet but maintaining it at 3 - 4mm thickness?
Not as far as I can tell and that's only because I've fused a few times and I have read the glass behaviour stuff (as you must have done from your post).
The only way that I think you could do this is to add some weight on top of the glass - put an extra kiln shelf on the top with "some" weights on it and then you could flatten it out, but I expect it would be unpredictable as to how thick it would be and also the final shape of the piece.
Be interested to hear if it's possible as well.
When I started going to evening classes in kiln work the tutor encouraged us to use float glass till we got used to cutting etc and I have a lot of pieces I made then using 2mm glass - they do not have as nice rounded edges but were not a total disaster. I have just made some little trinket dishes - two layers of 3mm glass plus frit and though they are nicely rounded after slumping they do look slightly clumsily thick so I would be glad to hear what advice is given.
I frequently fire pieces that are much less than 6mm. I tend to use 6mm for pendants and jewellery as it keeps it's shape better when I'm using my full fuse program. You can layer up on a 3mm piece but the top layer glass will not always "sink in" fully and this may just mean the dish will be a little bumpy which can add character. Always fused the piece flat first and then slump into the dish mould after. If the pieces are less than 6mm on a full fuse the edges may loose their shape a little to but again this can add to the design.
Recently made some coaster using a 3mm piece and a 2mm piece and they can out beautifully.
I hope this helps and experimenting is the best bit.
x
Thank you for all your responses. Just found this really useful tutorial
http://fusedglass.org/learn/project_tutorials/kiln_pressed_glass
It really is a matter of experimentation and note-taking to avoid repeating mistakes... kiln differences, float/bullseye/ glass thickness, mould profile - all require taking into account: and then there's temperature and hold...
If it's any encouragement, we made shallow dishes/bowls from 4mm float, but had to stray significantly from the schedule supplied with the kiln (Nabertherm) in maybe a surprising way:
"as listed" 6mm Bullseye: up to 673deg and hold for 10 mins.
"as developed" 4mm float: up to 835deg and hold for 35 mins.
So, not very intuitive then!
Chas
Thanks for the pressed kiln glass link, dori!
They explain the technique really clearly, and I love the result.