Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Kilns => Topic started by: Sarah A on October 24, 2012, 03:16:23 PM

Title: Bead cube help please
Post by: Sarah A on October 24, 2012, 03:16:23 PM
I'm so excited my bead cube has just come. I ordered the rack and now don't know if I just sit it on the floor of the kiln or on top of the tile and stand? There doesn't seem much space to put it on the tile but I do want to damage the floor either. Hope someone knows the answer. Thanks so much
Title: Re: Bead cube help please
Post by: tinker on October 24, 2012, 03:18:42 PM
Hi Sarah
Congrats :D
I just put mine on the kiln floor - I suspect if you put it on the tile there would be no room to put things on the top level of the rack.
Title: Re: Bead cube help please
Post by: helbels on October 24, 2012, 03:50:12 PM
Hiya

I don't have the shelf or tile in my kiln at all, and just have the rack resting on the floor of the bead cube.
Title: Re: Bead cube help please
Post by: Sarah A on October 24, 2012, 03:59:54 PM
Thank you ladies. It's on the floor and now at temp woohoo