Hi,my partner is making me a kiln door, as i am starting to make larger beads,and i want to start selling then eventually,could anyone tell me what you use to fill it? is it fiber blanket?if not what is it and where can i buy it please,thanks Parin.
Yes fibre blanket is fine.
I have some over from a "project", the non aggressive type.
PM me with how much you need and your addy and I'll donate some to you.
regards Pete
;DThanks will go to shed tonite and measure it and will pm you with the size thanks again Parin.(ps let me know what you want for postage)
;DThe fiber blanket came this morning thanks,Parin.
Good, now we need pics of what you have done with it :D
Pete
:oWill do, but it might be a few weeks as Marks a bit slow,but if you want some pics it might speed him up a bit,Parin.