Frit-Happens !

Lampwork => COE 104 => Topic started by: Niki Gough on October 14, 2012, 09:32:04 PM

Title: Encasing Rods
Post by: Niki Gough on October 14, 2012, 09:32:04 PM
Hi,

This may be a silly question but I am going to ask anyway :) I am a complete newbie and am just looking to add some rods to my stash for encasing. Please can someone advise what would be good for a newbie on a HotHead. I am using 104 but don't actually know exactly what the glass is that I have as most of it was given to me.

Any help and advice would be appreciated
Title: Re: Encasing Rods
Post by: Trudi on October 14, 2012, 10:11:09 PM
Hi

If you're looking for just a clear then Effetre  006 its a good place to start.
Title: Re: Encasing Rods
Post by: Niki Gough on October 14, 2012, 11:01:55 PM
Thanks Trudi