Technical Forum => Studio/workspace/setup/equipment => Kilns => Topic started by: Jayne at Funky Glass on October 03, 2012, 07:34:57 PM

Title: Annealing A Pile Of Beads
Post by: Jayne at Funky Glass on October 03, 2012, 07:34:57 PM
So, I have a pile of beads which are off the mandrels - how do I anneal them now?

Thanks for the support guys! Bear with me - I am blonde!

LoL
x
Title: Re: Annealing A Pile Of Beads
Post by: Glyn Burton on October 03, 2012, 07:57:27 PM
What sort of kiln do you have and what controller.
Title: Re: Annealing A Pile Of Beads
Post by: ♥♥Tan♥♥ on October 03, 2012, 07:59:33 PM
http://www.frit-happens.co.uk/forum/index.php?topic=859.0

Any good?
Title: Re: Annealing A Pile Of Beads
Post by: Jayne at Funky Glass on October 04, 2012, 08:09:15 PM
Thanks Tan..... I followed it and the kiln is in full swing!

:D
Title: Re: Annealing A Pile Of Beads
Post by: chipperpottery on October 05, 2012, 08:43:49 AM
Thanks Tan that is useful for me as well.
Title: Re: Annealing A Pile Of Beads
Post by: ♥♥Tan♥♥ on October 05, 2012, 11:20:48 AM
Yay, good news girls, lots of luck :-* ;D
Title: Re: Annealing A Pile Of Beads
Post by: Jayne at Funky Glass on October 05, 2012, 11:04:26 PM
Am on my third firing and so far so good  :D