Lampwork => COE 104 => Topic started by: Kimster on August 17, 2012, 02:33:49 PM

Title: dichroic noodles
Post by: Kimster on August 17, 2012, 02:33:49 PM
OOhh they've just arrived, dying to have a play about, any advice? Would the annealing prog still be the same as for other 104? Any guidance welcome! :)
Title: Re: dichroic noodles
Post by: Trudi on August 17, 2012, 06:48:20 PM
Hi  - if they're coe 104 then yes. Make sure you keep the coated side out of the flame!

Have fun.
Title: Re: dichroic noodles
Post by: Princess Peggy (Priscilla McGirr) on August 17, 2012, 09:20:14 PM
Use them like stringer...they're great!
Title: Re: dichroic noodles
Post by: Jellybean on August 17, 2012, 09:56:29 PM
Mine are in itsy bitsy pieces  :-[ can i just put little bits on with tweezers? I have a few bits which are a little longer I can use like stringer, but it won't go far...
Title: Re: dichroic noodles
Post by: Princess Peggy (Priscilla McGirr) on August 18, 2012, 09:44:31 AM
You can put little bits on, but heat the glassy side first if you can work out which it is and then turn them over and drop them on heated side up.
Title: Re: dichroic noodles
Post by: Trudi on August 18, 2012, 09:49:50 AM
I've never tried the noodles as I was concerned that they weren't fire polished ... might have ti give them a go!