This handy chart shows the reactive potential of Bullseye glass ..
http://www.bullseyeglass.com/images/stories/bullseye/PDF/other_technical/reactive_potential_of_bullseye_glass.pdf?utm_med
Ooh, likey!
Thanks for that, Bee.
I am dabbling with Bullseye, and this will be very useful
Linda x
I haven't used much Bullseye yet but I thought it was a useful chart to have for when I do!