August 05, 2012, 11:35:55 AM
My clear glass turned into a smoky grey, have I got it too hot?
>:(
Title:
Re: Clear glass
Post by:
Dragonfire Glass
on
August 05, 2012, 12:27:00 PM
Possibly, but more likely too much propane in the flame, or melting too close to the yellow candles :)
Title:
Re: Clear glass
Post by:
Magpie
on
August 05, 2012, 12:31:04 PM
Or running low on gas.