Lampwork => COE 104 => Topic started by: Kimster on July 21, 2012, 05:48:01 PM

Title: sand colour glass?
Post by: Kimster on July 21, 2012, 05:48:01 PM
Could anyone suggest a few 104 glasses to try that are a really good natural sand colour? All the ones I've tried have been too yellow/too cream/too streaky...before I spend even more money!  :D Cheers m'dears, hope you've all got some of this lovely sunshine   :)
Title: Re: sand colour glass?
Post by: Jellybean on July 21, 2012, 06:11:05 PM
silly question, but what sort of sand colour?!  north and south coast Cornish sand is different... what have you tried that you don't like? What do you want to do with it? I've got a few pale ones, and CIM Linen coming soon, if you want to pinch a few bits to try....  ;D
Title: Re: sand colour glass?
Post by: Kalorlo on July 21, 2012, 08:52:37 PM
Ivories no good? Light ivory will stay fairly unstreaky. I've got a whole load of beigy Lauscha colours, and there's CiM stoneground.

It really depends on the shade!
Title: Re: sand colour glass?
Post by: Dragonfire Glass on July 21, 2012, 09:57:18 PM
sansdstone?
Title: Re: sand colour glass?
Post by: Nikki on July 21, 2012, 10:14:59 PM
I have a couple of rods of one called caramel I think its Reichenbach if that would be any use,  its a dark sand colour but don't use it next to Ivory as it goes purple. ;D
Title: Re: sand colour glass?
Post by: Kimster on July 21, 2012, 11:02:36 PM
 I've tried both ivories (too streaky/creamy), stoneground (too yellowy), cool fossils (streaky again) , caramel (bit orangey)... haven't come across Sandstone Fallariel - d'you know who makes it? Sounds like the obvious one! Thanks for the kind offers too - might have to take you up on those!  :D
Title: Re: sand colour glass?
Post by: Dragonfire Glass on July 22, 2012, 12:11:54 AM
Have a look here

http://www.frit-happens.co.uk/forum/index.php?topic=27952.0


Title: Re: sand colour glass?
Post by: Jellybean on July 22, 2012, 07:45:24 AM
I have sandstone Kim if you want to pinch a bit  :)
Title: Re: sand colour glass?
Post by: Kimster on July 22, 2012, 04:25:34 PM
Thanks Emma & Fallariel - the 'sandstone' is just what I'm looking for! Does anyone have any to sell or know where I can buy some? Tried Tuffs, Off Mandrel etc websites & none there  :(

Emma if you have a rod or two that would be great! Thank you  :)