Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: jeannette on July 15, 2012, 01:14:05 PM

Title: Whoopsie - too close
Post by: jeannette on July 15, 2012, 01:14:05 PM
(http://farm9.staticflickr.com/8006/7574080928_f819629fdc.jpg) (http://www.flickr.com/photos/72286387@N07/7574080928/)
Untitled (http://www.flickr.com/photos/72286387@N07/7574080928/) by Jeannette Copeland (http://www.flickr.com/people/72286387@N07/), on Flickr
Doh!

And double doh for the image
Title: Re: Whoopsie - too close
Post by: Flyingcheesetoastie on July 15, 2012, 01:34:14 PM
Can't see the image....
Title: Re: Whoopsie - too close
Post by: BeeBeads on July 15, 2012, 01:36:56 PM
Dying to know what you were too close to!   :D
Title: Re: Whoopsie - too close
Post by: Zeldazog on July 15, 2012, 02:03:06 PM
Jeanette, you need to use the URL that "Grab the BB Link" gives you
Title: Re: Whoopsie - too close
Post by: Zeldazog on July 15, 2012, 02:03:22 PM
Ooops cross posted!

And, oopse, see what you mean about too close!  Shame, big chopping board??
Title: Re: Whoopsie - too close
Post by: jeannette on July 15, 2012, 02:06:10 PM
Big cheese server I'm thinking...dunno - took me ages to get through that hendrick's gin as well!
I was just being too greedy with the ginger beer bottle....
Title: Re: Whoopsie - too close
Post by: Margram on July 15, 2012, 02:34:11 PM
That looks quite usable - think you've started a new craze - soon everyone will be making them! :)
Title: Re: Whoopsie - too close
Post by: Blue Box Studio on July 15, 2012, 03:19:04 PM
In our house that would be cheese, butter and pickle.  I think it's very usable.
Title: Re: Whoopsie - too close
Post by: BeeBeads on July 15, 2012, 03:45:51 PM
I agree - very useable.  I think they look great, ideal for cheeses etc.
Title: Re: Whoopsie - too close
Post by: Pat from Canvey on July 15, 2012, 05:18:42 PM
It's all a learning experience. Now you won't do the same thing again unless you want a similar cheeseboard. At least you dodn't let the glass spill over the shelf  ;)  ;)  ;) Now you'll have to drink some more gin to try again. Shush, when the kids were small I used to get them to retrieve Harveys Bristol Cream bottles from the local bottle bank.
Title: Re: Whoopsie - too close
Post by: chipperpottery on July 15, 2012, 05:20:43 PM
I have done the same thing in the past
Title: Re: Whoopsie - too close
Post by: Nicknack on July 15, 2012, 05:31:58 PM
I've had the same sort of thing happen, leaving dichro pieces too long in the microwave kiln when I was starting.  Too big for a pendant, too small for anything else :(  I managed to break/cut pieces off, and refire to polish - saved some of it :)

Enjoy your cheese/butter/cracker board, it's original!!!!!!!!

Nick
Title: Re: Whoopsie - too close
Post by: nuttybeader on July 15, 2012, 07:57:07 PM
Serendipity I think it is called.  A new craze is born.  I can only do small bottles in my kiln and if I am not careful they go over the edge.