Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Tools and Presses => Topic started by: Kimster on July 06, 2012, 04:28:30 PM

Title: brass or graphite bead roller?
Post by: Kimster on July 06, 2012, 04:28:30 PM
I'm looking to splash out & buy one of these soon  :) but I need some advice!  As a beginner would I be better off with graphite or brass? Does anyone have one for sale? (The one with several different sizes of round beads). Does it make it harder to use if it doesn't have a mandrel groove? I've tried to contact Pegasus but can't get hold of them. If someone could point me in the right direction for suppliers that would be great. Thanks all!
Title: Re: brass or graphite bead roller?
Post by: garishglobes on July 06, 2012, 04:47:50 PM
There is some good information about graphite vs. brass rollers in this thread:

http://www.frit-happens.co.uk/forum/index.php?topic=37780.0 (http://www.frit-happens.co.uk/forum/index.php?topic=37780.0)

I would have thought it would help to have a mandrel groove for beads, but it is a long time since I've made beads so I'm just guessing this one!!
Title: Re: brass or graphite bead roller?
Post by: Blue Box Studio on July 06, 2012, 04:49:48 PM
Pegasus will reply, give them a day or two.  I think from the last reply I had they are back in production and Bev is on the road to recovery; but I think things are moving slower than normal.  I bought a bead shaper the other day and it was delivered within 48 hours, so some things are happening fine.
Title: Re: brass or graphite bead roller?
Post by: Calico Cat on July 06, 2012, 05:05:15 PM
The ones without mandrel slots are for making marbles (no mandrel involved).

Personally, I've always found the graphite rollers easier to use - but be careful, they get very, very hot - Mind where you put them down - I frequently singe my elbow leaning on one I've just used!