Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Studio/Workspaces => Topic started by: Kimster on June 10, 2012, 05:54:59 PM

Title: Storing/labelling stringers
Post by: Kimster on June 10, 2012, 05:54:59 PM
What does everybody do?  :-\
Title: Re: Storing/labelling stringers
Post by: helbels on June 10, 2012, 05:56:31 PM
I don't bother labelling, anything that's long enough to keep just gets put in a pot and then any short bits either get put in the bin or remelted onto the rod they came from (if I'm feeling organised).
Title: Re: Storing/labelling stringers
Post by: Shirley on June 10, 2012, 05:58:01 PM
I have a couple of racks of testtubes. Mostly I print a label for each colour and stick it on the tube. Tend to use it mostly for stringers that are silver glass, intense black or silvered. Most other colours I melt back onto the original rod and then repull as required.
Title: Re: Storing/labelling stringers
Post by: BeeBeads on June 10, 2012, 06:01:03 PM
Mine lie on the side of the desk so I can grab one when I need it.  They aren't labelled, just in a random pile!
I do keep SIS and intense black stringers in a separate pot on a shelf though.

My bought stringers are in a jar on the windowsill in front of the torch but they are much bigger than the ones I make.
Title: Re: Storing/labelling stringers
Post by: Katiequiggle on June 10, 2012, 09:51:16 PM
Mine are bunged in a couple of jam jars though I usually make them as I need them for each project and only keep them if they're long enough to re-use on something.
Title: Re: Storing/labelling stringers
Post by: Jellybean on June 10, 2012, 09:59:19 PM
jam jar for long stringers, small pot for short usable bits, and another small pot for twisties and silver glass  ;D
Title: Re: Storing/labelling stringers
Post by: Calico Cat on June 10, 2012, 10:08:58 PM
Ones that I have pulled myself go in a tall, skinny glass vase.

A selection of commercial ones are in what is supposed to be a stand for paintbrushes - a couple of pounds in The Works. The main stash of commercial ones - a lot of CIM ones from the US - go in very small waste pipe - mini versions of the pipe I keep rods in.

You may be relieved to know, I don't label any of them . . . . .
Title: Re: Storing/labelling stringers
Post by: Pam on June 10, 2012, 10:20:43 PM
I'm a jam jar stringer storer too. No labels
Title: Re: Storing/labelling stringers
Post by: spexy on June 10, 2012, 10:37:00 PM
Plastic test tubes from Ebay for me.
Title: Re: Storing/labelling stringers
Post by: Kimster on June 10, 2012, 11:03:36 PM
That's all reassuring. Mine are all in 3 jamjars.. (commercial, home made, silvered ivory) - just wasn't sure whether it's important to remember what exact glass they are - would be relatively easy to remember today since I just had a marathon pulling session (!) , rather than tomorrow when I know I won't be able to tell my smurfy from my ming (as it were!)  :o  ;)
Title: Re: Storing/labelling stringers
Post by: Blue Box Studio on June 10, 2012, 11:47:12 PM
All mixed together in a jam jar, or if too short to go in there I have a smaller pot.  Nothing is labelled.  I woldn't be able to tell my Smurfy from my Ming even if they were labelled (never had these colours as far as I am aware).  Apart from some clear and Ivory commercial stringers they are all mine and I like the element of surprise.
Title: Re: Storing/labelling stringers
Post by: Jellybean on June 11, 2012, 09:02:50 AM
ok newby question - why buy commercial stringers?
Please don't shout me down in flames, just wondering... for the sake of speed and convenience?
Title: Re: Storing/labelling stringers
Post by: MadelineBunyan on June 11, 2012, 09:46:42 AM
when I can be bothered, and I sometimes am for expensive colours or ones I use often, they go in glass test tubes I label with sharpie, I'll often put two very differernt colours in one test tube, then the test tubes go in a glass or jar.

as for the rest...rainbow spaghetti! it lives in a spaghetti jar, and a pasta sauce type jar or 3, and a glass...er, yes, I have too much stringer and I dont use the unlabelled stuff, I just pull new, I am bad. ::)

anyone want a jar of stringer? :D

commercial stringers are very thick, and even, which can be useful for some things (personally I dont use them) also some of the transparent colours scum quite easily when you pull them into stringer, so ready done could be quite useful.

if you want to pull your own thick stringer, the easiest method is to use 2 rods of the same colour or melt a longer rod apart in the middle, (and then stick it back together after.) this way you have both handles already attached and none of that dropping it
Title: Re: Storing/labelling stringers
Post by: ScarletLeonard on June 11, 2012, 10:14:59 AM
I pull mine then pop them in the tube with the matching rods.
silvered ivory has it's own tube, twisties tend to get used as they are made.

Anything too short to be found on the storage rack gets tucked into a mug.
Title: Re: Storing/labelling stringers
Post by: katherinem on June 11, 2012, 10:44:36 AM
I only keep SIS, twisties and cane - everything else is in a pile, and periodically I clear them into a box and forget about them! I've only just started using silver glass, so I tend to only pull very short stringers of that for now and use it all in one go.

The ones I keep are in mini egg tubes, they seem to be a perfect size - a good excuse for my DH to eat some more next Easter  :)
Title: Re: Storing/labelling stringers
Post by: Blue Box Studio on June 11, 2012, 06:31:09 PM
Quote from: Jellybean on June 11, 2012, 09:02:50 AM
ok newby question - why buy commercial stringers?
Please don't shout me down in flames, just wondering... for the sake of speed and convenience?

Came with my basic kit if I remember rightly.   
Title: Re: Storing/labelling stringers
Post by: Calico Cat on July 08, 2012, 07:11:53 PM
Just found these really cute little vases in IKEA - they might make good colour coded stringer storage!

(http://farm8.staticflickr.com/7136/7529058802_913a53ba6a_m.jpg)


http://www.ikea.com/gb/en/catalog/products/80215577/ (http://www.ikea.com/gb/en/catalog/products/80215577/)
Title: Re: Storing/labelling stringers
Post by: BeeBeads on July 08, 2012, 08:01:13 PM
Those little jars are lovely, what a good idea re the colour coding, and they're so cheap as well!
Title: Re: Storing/labelling stringers
Post by: squirsygirl on July 08, 2012, 08:55:08 PM
Quote from: Jellybean on June 11, 2012, 09:02:50 AM
ok newby question - why buy commercial stringers?
Please don't shout me down in flames, just wondering... for the sake of speed and convenience?

Why would we do that?   ???   ;)

Commercial stringers are especially made for us nupties who can't pull evenly sized ones.  (i.e. me).

And I always but intense black in stringers.

And they are pretty!   ;D
Title: Re: Storing/labelling stringers
Post by: mutti on July 08, 2012, 08:55:51 PM
Test tubes in a stand (unlabelled).  I work at a Secondary School as their permanent supply teacher.  The Science dept is brill.  I use a test tube holder/clamp as a short rod clamp - end up with just 1cm of rod that I chuck in a pot.  All free of course  ;)