What size mandrel do you guys use to make a cab on?
I have a cab mandrel but fancy trying to make one 'Patti Walton' style (at the Flame Off this year). I've tried a 5mm and the bead release fell off before I even got started (too cool, I guess) and a 2mm - managed an ok cab at the end but it was wobbling furiously by the time I plonked it onto the bottom of the kiln  ;D
So, for those of you that do...... What size and any tips?
Thanks guys  ;D
Title: Re: Making a cab on the end of a mandrel
Post by: sparrow on May 31, 2012, 08:24:57 AM
I usually make them on 2mm mandrels....but not as big as Pati!  ;D
Title: Re: Making a cab on the end of a mandrel
Post by: Margram on May 31, 2012, 08:36:20 AM
Yes, 2mm - and keep warming the back! :)
Title: Re: Making a cab on the end of a mandrel
Post by: julieHB on May 31, 2012, 08:41:01 AM
I almost always use 2.4mm - just a tad sturdier than the 2mm, but not so big that it draws the heat out of the glass to quickly.
Title: Re: Making a cab on the end of a mandrel
Post by: MangoBeads on May 31, 2012, 09:00:59 AM
Any size but the bigger the mandrel anchor the glass further down the tip so more of the mandrel is inside the cab . Does that makes sense ?
Title: Re: Making a cab on the end of a mandrel
Post by: mizgeorge on May 31, 2012, 12:01:14 PM
Julie's beadspanner makes these a whole lot easier too!
Title: Re: Making a cab on the end of a mandrel
Post by: Donna@Rockin' Beads on May 31, 2012, 06:11:19 PM
Excellent. So, really I just need to practise  ;D
Your bead spanner looks great Julie, maybe you'd like me to stock it in the shop for you  ;D ;D
Title: Re: Making a cab on the end of a mandrel
Post by: Krysia@No98 on May 31, 2012, 06:39:45 PM

Maybe look at your bead release too, is it too thick?
Title: Re: Making a cab on the end of a mandrel
Post by: SilverGems89 on May 31, 2012, 06:42:40 PM
I use 2.4mm mandrels for cabs also, if it's wobbling your working too hot  :P
Title: Re: Making a cab on the end of a mandrel
Post by: Donna@Rockin' Beads on May 31, 2012, 07:16:10 PM
I dont think it was wobbling because it was too hot. I think I wasn't quite gentle enough  :)
Title: Re: Making a cab on the end of a mandrel
Post by: SilverGems89 on May 31, 2012, 07:54:56 PM
Quote from: Donna@Rockin' Beads on May 31, 2012, 07:16:10 PM
I dont think it was wobbling because it was too hot. I think I wasn't quite gentle enough  :)

ahhhhh, yeah, i always use fresh dipped and flame dried mandrels for cabs  ;D
Title: Re: Making a cab on the end of a mandrel
Post by: Donna@Rockin' Beads on May 31, 2012, 08:13:34 PM
Great tips. Thank you.
Title: Re: Making a cab on the end of a mandrel
Post by: JKC on May 31, 2012, 09:09:29 PM
I use 1.6 mandrel for stud earrings. Janet
Title: Re: Making a cab on the end of a mandrel
Post by: Lush! on May 31, 2012, 11:18:46 PM
I like big ones ... mandrels, that is  ;D
Title: Re: Making a cab on the end of a mandrel
Post by: Diane on June 01, 2012, 10:22:39 AM
QuoteI like big ones ... mandrels, that is

Well someone had to lower the tone ::) ;D ;D ;D
Title: Re: Making a cab on the end of a mandrel
Post by: Donna@Rockin' Beads on June 01, 2012, 11:16:55 AM
 ;D ;D ;D