Beside myself with excitement & can't wait to have a go with my Kilncare Ace! Just read the instructions & it says use fibre paper to put my beads on....where do you recommend I get this from & do I definitely need it? Any advice welcome as usual (just noticed I have 2 stars & am not a newbie any more..that is so not true! How did that happen? Don't want to be 'promoted' up with the big girls before my time!!)
I have a wire mesh which I poke the mandrels into. On the base of the mesh I have a fibre blanket pad thing that came with my kiln.
The mesh is easy to shape and will keep your beads off the base of the kiln but some sort of protection is recommended anyway in case of melting incidents (never had one, phew).
I think if you are batch annealing then a lot of people just pile the beads in a dish.
If you are garaging then you can get a mandrel rest for the kiln from Tuffnells (woud think the one for the SG2 will fit)
As for the stars the more you post the more stars you get ;D ;D ;D ;D
Quote from: poledra1958 on May 24, 2012, 03:51:17 PM
I think if you are batch annealing then a lot of people just pile the beads in a dish.
Thanks Jenny. Another dumb question, what should the dish be made out of ?! ::)
No need for fiberpaper for beads, if you are going to do slumping in there then you will need fiberpaper bla bla bla :)
Because when the beads go in the kiln they will not be melty they will be in solid form.
Quote from: Kimster on May 24, 2012, 04:48:25 PM
Thanks Jenny. Another dumb question, what should the dish be made out of ?! ::)
a pirex dish from wilkos will be fine, nothing fancy
I think some folk use plain old terracotta dishes :)
Cross posted Krysia :D
;D
If you want to be super careful, a plain white tile will do on the bottom of the kiln.
These are all just precautions, if something goes wrong and the temperature gets too high and your beads melt into a big puddle they wont stick and ruin your shelf, so no you don't necessarily need fibre paper (which is quite expensive) any of the other suggestions in this thread will be just as good (and probably cheaper!)
I use an old pyrex bowl for my soft glass beads
Ready to have a go now - gawd - just to check, I have 89 beads all piled up in a glass bowl which I hope is pyrex! Is it OK that they're all on top of each other & touching each other? ??? ???
Can I add a word of caution. I batch annealed all the beads I had been making from when I started, a big pile in a pyrex bowl and they all stuck together. I had a lot of beads with Rubino and some Iris orange which broke into bits. I did have the correct temperature settings.
I would do them kebab style on short mandrels.
I do the same as Linda Spexy, on short mandrels - great for using up your bent and mangled ones!
I've never tried the Pyrex bowl method so can't comment.
And I use kiln shelf paper on the shelf and the floor of the kiln, just as a precaution ;)
I'm still using the huge sheet that I bought with the kiln, years ago. Just cut it to size and you can use it for more
than one firing so it's not as expensive as you think.
Best of luck, the first firing is very exciting!
Quote from: spexy on May 25, 2012, 08:52:48 AM
Can I add a word of caution. I batch annealed all the beads I had been making from when I started, a big pile in a pyrex bowl and they all stuck together. I had a lot of beads with Rubino and some Iris orange which broke into bits. I did have the correct temperature settings.
I would do them kebab style on short mandrels.
Unusual - I've batch annealed for about 5 years now, used the same pyrex bowl and never had this happen... ???
When I got my kiln and I was doing the first batch annealing run I did it with all my utter fuglies that way if something went wrong it wouldn't be a disaster then I did the not so fuglies.
I've only had beads that I have put in too hot straight from the flame stick to each other.
GOOO-AAARRRNNNNN Kimster. Go for it matey. ;D
Quote from: Lee - Kilncare on May 25, 2012, 12:13:27 PM
GOOO-AAARRRNNNNN Kimster. Go for it matey. ;D
;D ;D
All back on mandrels now!!!
Kiln on, heating up the room nicely ::)
wow Kim I'm impressed you're doing it in this heat!!! I had to stop yesterday because I was melting!!
I want to see the results - so exciting!! ;D
Oooh so exciting! Kiln has finished its cycle (finally!) Felt like I was starting to get annealed myself in the heat... ;D
The temp went down to 250... have just had a peek & all 89 beads still look intact... am I allowed to get them out yet, or do I wait till everythings gone back to room temp in the kiln - feels quite hot in there still, mind you so does my house ;D
wait wait wait!!! it's the agonising wait now.....
I usually wait until it's room temp by going to bed (early if necessary!!!) but I have got things out at 45C
Patience now.... ;D
I've opened the door at around 100 and taken out when they aren't burny hot to touch - probably about 60. I don't even peek until they get down to 100 though!!!
Dammit!! I opened the door about 5 times after they got down to 250, cos the program said 'end'.. :-[ How will I know if they're OK? If they don't crack? They're now on about 70....
time for a glass of wine then....
clean them with a dremel, if they survive that, they'll survive anything. But if some break, then they break and always will no matter how long you've been at making beads.
I tend to open my door at 100 too. I would say that 250 probably isn't fatal, but doing to putting them in a metal bowl until they have been at room temperature.
ohhh I'm very impressed that you have got as far as firing with it .... I've yet to work out how to do the initial firing - but then again I'm a techno-retard.
Any tips would be gratefully received.
the best advice I can give you it to ring the supplier and get them to talk you through the programming. I didn't manage it and I would not consider myself technically challenged. The supplier won't mind the call.
Quote from: toodlesandbinks on May 27, 2012, 08:07:56 PM
ohhh I'm very impressed that you have got as far as firing with it .... I've yet to work out how to do the initial firing - but then again I'm a techno-retard.
It was all programmed for me by Lee at Kilncare...all I had to do was bung them in, switch on & press prog 1 or 2. And I still had 101 questions about it!! I ended up with 88 beads intact, only 1 cracked...but haven't yet dared clean them with a Dremel (only by hand...) Is yr kiln from Kilncare?
I realised that it was programmed in and it didn't need an initial firing after I spoke to Lee.
Glad you had such good results, I am just working on getting something to anneal with mine.
Keep up the good work gals :D