Lampwork => Lampworking Tip n Tricks => Topic started by: lantana on May 01, 2012, 01:00:13 PM

Title: Goldstone ribbons
Post by: lantana on May 01, 2012, 01:00:13 PM
Hi all, I have just taken delivery of some goldstone ribbons, and although I have used goldstone frit before, I'm not sure whether they should be made into smaller stringers or used as they are? any advice would be welcome. Thanks  :D
Title: Re: Goldstone ribbons
Post by: tsarvo on May 01, 2012, 01:06:15 PM
Good question, I tried them for the first time yesterday.
I have to admit that I lost almost half of the first rod as it shocked all over me
(aleast I looked sparkly pretty but not huggable :-) )
Attempted to pull it into stringers which wasn't a huge success :-0
But a lot of what I tried yesterday wasn't great. X
Title: Re: Goldstone ribbons
Post by: julieHB on May 01, 2012, 01:09:20 PM
I just use them as they are; work cool if you want to keep the sparkle  :)

It is easier to keep the sparkle if you encase it, but still wouldn't blast it with heat.
Title: Re: Goldstone ribbons
Post by: lantana on May 01, 2012, 01:23:51 PM
Thanks, I will try it as is. It just looks quite wide, and if I just wanted a little sparkle, say behind some flowers, will it be too much? Could it be applied onto a clear rod and pulled into a thin stringer I wonder  :)
Title: Re: Goldstone ribbons
Post by: Trudi on May 01, 2012, 01:58:48 PM
Are you working with flat goldstone ribbons or encased goldstone rods?


I find the commercial rods very shocky and prefer to make my own stringers! It's very easy and you can have them as thick or thin as you like!
Title: Re: Goldstone ribbons
Post by: ARBeads on May 01, 2012, 02:05:59 PM
I'm with Trudi on this - pull you're own using light Amethyst to increase the sparkle.

I tried the pre pulled blue stringer and found it to incompatible with most Effetre - pinging of both immediately after annealing and several weeks later - yes the stringer was well attached to the base bead - it's almost like it's incompatible with itself!
Title: Re: Goldstone ribbons
Post by: lantana on May 01, 2012, 02:31:25 PM
Trudi - they are ribbons and quite wide. How would I make my own? :D
Title: Re: Goldstone ribbons
Post by: Kathy on May 01, 2012, 04:58:16 PM
Ooh, I'd love to know that too - I got a couple of ribbons in a swap a little while ago and never known what to do with them! :D
Title: Re: Goldstone ribbons
Post by: Madam Steph on May 01, 2012, 05:16:37 PM
I think Trudi means to pull your own stringer..not your own ribbons


I could be wrong


Linda x
Title: Re: Goldstone ribbons
Post by: noora on May 02, 2012, 08:23:39 AM
I have some bluestone ribbons (Tuffnell's sent them as replacement when I had ordered bluestone stringers but they were out) and just apply them as they are. Looks nice when you wrap some all the way around a bead and encase. It adds a nice sparkle. That's the only use I've found for them so far, they're too wide for small dots or scrollwork. The blue/purple ones to the right in this photo have some bluestone ribbon applied like that, perhaps you can see a bit of the sparkle in the photo:

(http://www.rangifer.se/exp_img/bhbeads.jpg)
Title: Re: Goldstone ribbons
Post by: julieHB on May 02, 2012, 08:33:32 AM
You can pull the ribbon into thinner stringer if you want - just work cool.

If you want encased stringer you can encase a bit of the ribbon thinly before pulling it out to an encased stringer. To get a really thin encasing pull thick stringers of the clear glass to encase with.

Alternatively you can buy goldstone nuggets that you encase and pull stringer from. Add a bit of clear glass onto the end of a mandrel, heat until molten and fix to a lump of goldstone which has been pre-warmed. Encase and pull into stringer.
Title: Re: Goldstone ribbons
Post by: sarah t on May 02, 2012, 08:46:29 AM
you can use the ribbon on its side rather than flat ( holding it like a pencil) for thinner lines and dots
Title: Re: Goldstone ribbons
Post by: james M knox on May 02, 2012, 10:17:23 AM
Hi All,

I find these ribbons make very nice twisties. 

I Melt a blob of white glass and mash it into a lollypop.

the gently melt the blue or gold ribbon on one side of the lollipop.

carefully cover the blue ribbon with either clear or a pale blue transparent.

cover the other side of the lollipop with some contrasting colour, I sometimes use red/orange or turquise.

Encase all the covered lollipop in thin clear,

Heat, pull and twist - Nice twisty with the goldstone shimmer.

This looks nice with the blue on one side and the gold on the other as well.

JMKnox
Title: Re: Goldstone ribbons
Post by: Redhotsal on May 02, 2012, 10:27:48 AM
Nice tip James, - goldstone also looks great encased in rubino.
Title: Re: Goldstone ribbons
Post by: julieHB on May 02, 2012, 11:30:53 AM
Quote from: Redhotsal on May 02, 2012, 10:27:48 AM
goldstone also looks great encased in rubino.

Oooooooh - haven't tried that - sounds very nice!

James, thanks for that great twistie recipe!
Title: Re: Goldstone ribbons
Post by: lantana on May 02, 2012, 03:04:58 PM
ooh, thanks for the tips, I have had some success today using them on their side to trail. Will post some pics later  :)
Title: Re: Goldstone ribbons
Post by: lantana on May 02, 2012, 06:27:00 PM
I have had some success today, this was one of 3, the other 2 cracked - grrrr. You can clearly see the goldstone. I used a black base.(https://lh3.googleusercontent.com/-gKTsqHP6cVY/T6FuQTJADoI/AAAAAAAAAOY/kCP58rEVD-I/s912/IMAG1211.jpg)
Title: Re: Goldstone ribbons
Post by: SRJ on May 11, 2012, 08:07:16 PM
Lantana - That is lovely!
Title: Re: Goldstone ribbons
Post by: Margram on May 11, 2012, 08:26:56 PM
It is! :)
Title: Re: Goldstone ribbons
Post by: Glyn Burton on May 11, 2012, 08:53:47 PM
I always make my own goldstone stringers, its cheaper and you can make them as thick or thin as you like. Lumps of goldstone from Martin are quite cheap and last ages. Chip a bit off the lump with a hammer warm it in the back of the flame and stick it on to a rod, encase and pull out to required thickness. Simple as that.
Title: Re: Goldstone ribbons
Post by: Redhotsal on May 11, 2012, 10:49:29 PM
....But don't do what I did when I first started beadmaking and dunk a massive big lump of it straight into the flame. I spend an unhappy evening picking the bits out of my face. Preheating the larger lumps in the kiln will work much better.
Title: Re: Goldstone ribbons
Post by: Dee Dee on May 12, 2012, 01:10:54 AM
The bead is lovely!  Some great tips too, like the twisty idea, and I have never thought of encasing goldstone with rubino - definitely something to try!  Anyone got any pics of these??
Title: Re: Goldstone ribbons
Post by: jammie on May 12, 2012, 10:45:25 AM
great ideas here thanks...I've made the goldstone stringers but not tried with light amethyst, and have the bluestone ribbons but wasn't having much luck with them so will try the ideas here too!  :)
Title: Re: Goldstone ribbons
Post by: Kathy on May 13, 2012, 11:43:20 AM
I've made some stringers encased in Rubino after seeing this thread - but haven't tried them yet!!! :D Will let you know the outcome ;)