If you have a stuck bead, soak the bead and mandrel in descaler.

I had two that were completely stuck, hot water, cold water, freezer, pliers, vice - noting was budging them.

I had some descaler under the sink, £1 ish from Savers, or Wilcos or somewhere, so I thought, I'll give it a go. 

20 mins later - they slid right off.

Could've been a coincidence, but it may be worth a try.
Title: Re: Oo, look what I found...! out
Post by: awrylemming on April 26, 2012, 07:37:34 PM
Ah, I have both descaler and stuck beadies, time to play ...
Ta  :-*
Title: Re: Oo, look what I found...! out
Post by: noora on April 26, 2012, 08:13:06 PM
Neat! Must try!  :)
Title: Re: Oo, look what I found...! out
Post by: spexy on April 26, 2012, 08:23:21 PM
Thanks for sharing.
Title: Re: Oo, look what I found...! out
Post by: JanT on April 26, 2012, 08:51:00 PM
Thanks for the tip will try that next time I think the hammer is the only answer ;D