Frit-Happens !

Lampwork => Common Problems => Topic started by: Krysia@No98 on April 16, 2012, 10:12:27 PM

Title: Presses: Big lentil types
Post by: Krysia@No98 on April 16, 2012, 10:12:27 PM

I have been working this afternoon with my new 40mm lentil/coin press.  I'm finding it cracks a lot.  >:(

I warm the bead press it and it cracks!?!

Is there some additional trick like keeping the press warm that I should know about?

Thank you
Title: Re: Presses: Big lentil types
Post by: Kaz on April 16, 2012, 10:24:32 PM
The bead needs to be warmer - if the middle has gone cool it may crack while you're working it. Just reheat thoroughly and then repress.
Kazx
Title: Re: Presses: Big lentil types
Post by: ScarletLeonard on April 16, 2012, 10:27:02 PM
I keep my presses on my torch top marver, keeps the press nice and warm too, but as Kaz said it is probably the middle of the bead getting to cool.
Title: Re: Presses: Big lentil types
Post by: sarah t on April 16, 2012, 11:15:43 PM
use a larger mandrel it maintains the heat better in the bigger beads at the core and then like the others say heat control is the key
Title: Re: Presses: Big lentil types
Post by: awrylemming on April 17, 2012, 07:35:59 AM
I keep my big presses on top of the kiln unless I'm using striking glasses and want it to be cold.  It lessens the thermal shock to the glass and I rarely lose a bead since I started doing this.
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on April 17, 2012, 08:19:48 AM

I have been using a thicker mandrel, a 2.4, I'm usually on a 1.6.

Interestingly the cracks have been appearing at 11 and 1

I have been getting worried that heating the bead too much before it's pressed will make it lose it's definition and I have only been repeatedly pressing because they have already started to loses that definition before hand....

Thank you I shall try these tips on wednesday or thursday when I next get to the torch  :-*
Title: Re: Presses: Big lentil types
Post by: Helen G on April 17, 2012, 10:13:36 AM
I have a 45mm or 50mm (can't remember which) slim lentil press and it is a b****r to use, I've had the same cracking/splitting issues and like Kaz said it is when the glass is a little too cool so rather than squish it splits :-\

I usually press gently several times on both sides  ;)
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on April 17, 2012, 01:30:03 PM

yup pressing more then once.

I'm fine with other presses.  Only have cracking issues with the Bavarian flat eggs and the flat heart but that's because they are so very thin...

It goes, load glass, make very melty, press, get part shape, make melty but not too much again, press again, now should be about the right shape, make almost melty for tidy up presses, do this a few times, all fine, so get to decorating...

If the bead needs to be pressed again then the cracking occurs, by this time the press has cooled down.
Title: Re: Presses: Big lentil types
Post by: Dragonfire Glass on April 17, 2012, 01:40:49 PM
you need to keep warming it whilst decorating ...
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on April 17, 2012, 03:09:52 PM

I am keeping it too warm while decorating which is why I go back to press it, in the mean time the press has got cold and that is what cracks the bead!!
Title: Re: Presses: Big lentil types
Post by: Pat from Canvey on April 19, 2012, 08:56:13 AM
I have never pre-warmed a press. The action of pressing warms it up anyway.
Title: Re: Presses: Big lentil types
Post by: sarah t on April 19, 2012, 10:35:04 AM
and if they get too warm the pins can stick ...i generally only use the top on the final couple of presses ,i shape and tweek using only the bottom of the press 
Title: Re: Presses: Big lentil types
Post by: flame n fuse on April 19, 2012, 12:27:08 PM
My pressed lentils often crack if they have transparent over an opaque core, but not the 11 and 1 pattern.
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on April 19, 2012, 01:03:21 PM
Quote from: sarah t on April 19, 2012, 10:35:04 AM
and if they get too warm the pins can stick ...i generally only use the top on the final couple of presses ,i shape and tweek using only the bottom of the press 

still cracks when I only use half of it  ::)  But I know what you mean about the sticking pins.

Think I am going to need to go back to the thursday principle of slowly when it comes to re heating after the decorating.

If it does the 11 and 1 cracks I shall see if I can get a picture.  It interesting that you should mention incasing I had put a naff glass on the inside and put the 'nice' glass over the top.
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on April 22, 2012, 07:02:38 PM


okey dokey, I put the press on the torch top marver and there were a lot less cracking issues.  However because I get stupidly close I nearly caught myself in the face a few times with a hot pin  ::)
Title: Re: Presses: Big lentil types
Post by: Magpie on April 22, 2012, 07:25:21 PM
I usually have the press on the torch top marver, mainly coz I then know I'm not going to stick my hand in the flame trying to get the top on the bottom!
Title: Re: Presses: Big lentil types
Post by: Josephine on April 23, 2012, 07:24:29 PM
Are you remembering to warm both sides of the bead, not just the side you are decorating. When I make my big tree beads I stop work on the decoration frequently and really bathe the back of the bead in the flame. I do it further out in the flame so the heat isn't to directed/intense then flip back to the side I'm working on.
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on April 23, 2012, 10:56:22 PM

Yup, and paying particular attention to the mandrel and round the edge
Title: Re: Presses: Big lentil types
Post by: Krysia@No98 on May 01, 2012, 11:37:47 AM

I do have a kiln,  I don't have this problem with smaller presses.

I generally make stuff on 1.6.  It feels really funny making stuff on bigger rods.

I have been heating along the line of the rod.

the problem isn't that it cracks as I first make the bead it's then I have been decorating it and popped it back in the press, between the time of making the original bead and then decorating it and then going back to the press the press has cooled down and takes far more heat from the bead and that causes the bead to crack, unless I get the bead all soupy which I really don't want as I've just decorated it then it will crack. I have found that putting the press on the torch top marver has helped the press retain the heat and makes it less likely to crack before I press it post decoration.