Title: Everything is brown ...
Post by: Lynnybobs on April 09, 2012, 10:01:32 AM
Had a torch session yesterday but very disapointed as everything came out brown or with streaks of brown  :( Effetre light sky blue came out worst but periwinkle was also streaky and I use this colour all the time with no problems. I tried working hotter and cooler but no real difference.
My only thought is that my gas is getting low so maybe something to do with that ? I'm on a hothead on bulk - any advice folks?
Thanks.
X
Title: Re: Everything is brown ...
Post by: Blue Box Studio on April 09, 2012, 10:21:53 AM
I had streaky beads when the gas got low on my hothead so could be that if not a problem you usually have.  But I was almost down to the last pffft when I got to this stage so ditched what was left and got a refill from the petrol station.

Am amazed how much longer gas lasts on a dual-fuel torch!  Would have been through several cylinders by now on my HH and still some left.  It's Murphy's revenge - I managed to get another (full) cylinder on Freecycle so I had a spare - in the autumn!
Title: Re: Everything is brown ...
Post by: cbeadies on April 09, 2012, 10:27:07 AM
this happened to me once when the gas was very low - made a beautiful orange polka dot heart with brown streaks!!  >:( I haven't had this problem since though so why it happened with that particular canister I don't know.
Title: Re: Everything is brown ...
Post by: Corinne Lacy on April 09, 2012, 10:31:14 AM
To find out how much gas is left pour a kettle full of boiling/just boiled water down the side of the gas bottle. The condensation mark/level shows what's left.
Hope this helps, does sound like you are running out though.

Corinne.
Title: Re: Everything is brown ...
Post by: flame n fuse on April 09, 2012, 10:33:40 AM
I had this problem with a HH on mapp gas when either the room was very cold, or the gas was running out.
Title: Re: Everything is brown ...
Post by: helbels on April 09, 2012, 10:50:53 AM
You could also try working further out... sometimes glass gets sooty if you are too close to the torch head on a HH.
Title: Re: Everything is brown ...
Post by: Blue Box Studio on April 09, 2012, 03:36:54 PM
I always knew when the gas was running out, I got closer and closer to the torch head!
Title: Re: Everything is brown ...
Post by: jammie on April 09, 2012, 04:23:13 PM
I got that, blue and white oh and clear show up worse, very likely low gas and also try giving the hot head a clean up as gunk might be stuck inside.
Title: Re: Everything is brown ...
Post by: Madam Steph on April 09, 2012, 06:25:06 PM
Quote from: Corinne Lacy on April 09, 2012, 10:31:14 AM
To find out how much gas is left pour a kettle full of boiling/just boiled water down the side of the gas bottle. The condensation mark/level shows what's left.
Hope this helps, does sound like you are running out though.

Corinne.

Corrine..I have just flooded my Loungio carpet  ::)

Linda x
Title: Re: Everything is brown ...
Post by: Pauline on April 09, 2012, 06:42:24 PM
Quote from: Madam Steph on April 09, 2012, 06:25:06 PM
Quote from: Corinne Lacy on April 09, 2012, 10:31:14 AM
To find out how much gas is left pour a kettle full of boiling/just boiled water down the side of the gas bottle. The condensation mark/level shows what's left.
Hope this helps, does sound like you are running out though.

Corinne.

Corrine..I have just flooded my Loungio carpet  ::)

Linda x

less likely to get scorch marks from molten glass then
Title: Re: Everything is brown ...
Post by: Corinne Lacy on April 09, 2012, 08:30:04 PM
Oh my goodness, you lot cheer me up every time I lurk on here!!!!

Corinne x
Title: Re: Everything is brown ...
Post by: Madam Steph on April 09, 2012, 10:12:29 PM
Quote from: Pauline on April 09, 2012, 06:42:24 PM
Quote from: Madam Steph on April 09, 2012, 06:25:06 PM
Quote from: Corinne Lacy on April 09, 2012, 10:31:14 AM
To find out how much gas is left pour a kettle full of boiling/just boiled water down the side of the gas bottle. The condensation mark/level shows what's left.
Hope this helps, does sound like you are running out though.

Corinne.

Corrine..I have just flooded my Loungio carpet  ::)

Linda x

less likely to get scorch marks from molten glass then

The puddle is merely hiding the molten glass marks.
They generally add a certain je ne sais quoi to my bijou set up  ;D

Linda x
Title: Re: Everything is brown ...
Post by: Lynnybobs on April 10, 2012, 09:22:02 AM
Hope your loungio had dried out Linda !  :) Looks like low gas is the problem - can't complain though as I've been using the same tank since the grand opening of the shedio back in August !
Looks like its stringer pulling practice - and bot I need it - for the time being until I can get an replacement - thanks everyone :)