Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: LampyLou on March 29, 2012, 10:46:24 AM

Title: Rubino and black dots?
Post by: LampyLou on March 29, 2012, 10:46:24 AM
OK so what am I doing wrong?  I'm trying to do some pink flowers over Appletini which should come out really dainty and pretty and but I keep getting little black dots on my rubino.  I've got the flame as low as I can and still melt (!?!) and I'm trying to work gently.  Any tips?

Thanks

Julia
Title: Re: Rubino and black dots?
Post by: Dee Dee on March 29, 2012, 10:48:11 AM
Are you putting your rubino over white dots??
Title: Re: Rubino and black dots?
Post by: LampyLou on March 29, 2012, 11:00:12 AM
I've got Effetre Pale Pink as the base of the petals, then Reichenback Opal Raspberry. The idea is to use the Rubino as the deep pink centre before I punge for my bubbles.

Thanks!

J
Title: Re: Rubino and black dots?
Post by: tish on March 29, 2012, 11:05:54 AM
i cann t help sorry still to new at all this but that sounds nice can u show us a piccy of them even with the black dots please
Title: Re: Rubino and black dots?
Post by: Dee Dee on March 29, 2012, 11:06:31 AM
Maybe try putting a dot of clear over the rubino??  Do you have any CIM cranberry?
Title: Re: Rubino and black dots?
Post by: sarah t on March 29, 2012, 11:09:51 AM
could be a compatability/reaction issue .....maybe clear inbetween the layers ?
Title: Re: Rubino and black dots?
Post by: LampyLou on March 29, 2012, 11:13:43 AM
Deedee, no I haven't any Cranberry, it's on my wish list but I always gasp at the cost.  I'll have another play and see if I can get the clear over.  Thanks.

Tish, I'm making them this morning (Coffee break at the mo!) so I'll try and show you either tomorrow or the weekend.  They are just simple handshaped doughnuts with 3 flowers, no exciting vine cane or anything.

Julia x
Title: Re: Rubino and black dots?
Post by: MyPrecious on March 29, 2012, 11:14:41 AM
Could it be the rubino reducing in the flame?
Title: Re: Rubino and black dots?
Post by: Dee Dee on March 29, 2012, 11:18:58 AM
Fingers crossed, that will help!  I think it might be reducing too, Kathy!
Title: Re: Rubino and black dots?
Post by: Madam Steph on March 29, 2012, 11:20:39 AM
Quote from: MyPrecious on March 29, 2012, 11:14:41 AM
Could it be the rubino reducing in the flame?
I'm sure that's what is happening, Kathy.
Same thing happened to me when I put it over some white dots on a large white heart I made a few weeks ago.

Yes, I found Cranberry was the way to go with this


Linda
Title: Re: Rubino and black dots?
Post by: Redhotsal on March 29, 2012, 11:56:39 AM
I agree with Kathy - it's reducing. You'll see the black dots "glowing" in the flame. The way to go with rubino is to lower the flame and work higher up. You can burn it very easily. It's a beautiful glass though if you persist and handle it carefully. Much better than cranberry if you ask me.

Rubino will react really badly with some colours - specifically ivory. It'll go a horrible grey if you dot it over that!
Title: Re: Rubino and black dots?
Post by: LampyLou on March 29, 2012, 12:01:23 PM
Thanks everybody!  I'll have another look at my flame.

Julia