Post by: Firo on February 05, 2012, 06:58:20 PM
Have just made some beads, fist attempt, which I'm quite pleased with but have only been able to get 2 off the mandrels. Tried freezing them, no joy, soaked in water, no joy so here I am asking for help. I think it may be duff bead release (bought 2nd hand off the person selling the kit) as when I opened it it was dry so I added a little water to make it into a paste. I'm now thinking that was wrong thing to do. Any ideas appreciated as the beads are pretty and would make a lovely necklace.
Title: Re: Beads are stuck on the mandrels ?
Post by: Madam Steph on February 05, 2012, 07:03:26 PM
This may sound elementary, and for that I'm sorry, but....do you have a decent pair of pliers with which to grip your mandrels when removing the beads?
Try soaking them again....try etching them...anything is worth a go.

Linda x
Title: Re: Beads are stuck on the mandrels ?
Post by: Purple Cobwebs on February 05, 2012, 07:09:47 PM
I often add water to bead release that has thickened, and after a good shake it's fine.
I soak my beads in warm water and washing up liquid to soften the bead release and then I use mole grips to grip my rods as they give an incredible firm grip. Some firm bead twisting then usually does the trick.
Title: Re: Beads are stuck on the mandrels ?
Post by: Blue Box Studio on February 05, 2012, 07:28:46 PM
Cillit bang apparently works, although never worked for me.  I usually leave to soak for 24 hours and then attack with my pliers.  If all else fails, and I get a few that refuse ever to budge, I either heat up (very carefully) then plunge in the water to save a mandrel, or use them as plant stakes.  I have a lot of plant stakes from my early days.
Title: Re: Beads are stuck on the mandrels ?
Post by: Firo on February 05, 2012, 07:29:14 PM
Tried the pliers and still they are not moving so will now try soaking in hot water with washing up liquid....
Title: Re: Beads are stuck on the mandrels ?
Post by: Firo on February 05, 2012, 07:31:24 PM
Still laughing at the plant stakes....lol
now wondering if they'd sell...lol
Title: Re: Beads are stuck on the mandrels ?
Post by: sea-thistle on February 05, 2012, 07:34:15 PM
If you have a vice, you could grip the mandrel in this putting the mandrel in lengthways and see if you can get the bead off that way, that's what I  have done when they are a bit stubborn coming off the mandrel
Title: Re: Beads are stuck on the mandrels ?
Post by: ★★Terri★★ on February 05, 2012, 07:50:52 PM


I've found the only Cillit Bang that works is the 'Grime and Lime' one.  The degreasing kitchen one doesn't do the job.

Like others have said - a good strong pair of pliers to grip the mandrel and a tea towel to grip the bead and usually they come off.

Title: Re: Beads are stuck on the mandrels ?
Post by: Angie on February 05, 2012, 07:57:50 PM
Try the plierslike everyone has said and twist the beads with a dry rubber glove on your hand.
Title: Re: Beads are stuck on the mandrels ?
Post by: helbels on February 05, 2012, 08:19:34 PM
In my experience, Mole Grips work much better than pliers.  I'd be lost without mine!
Title: Re: Beads are stuck on the mandrels ?
Post by: ScarletLeonard on February 05, 2012, 08:22:43 PM
It is possible though that the bead release broke when you were first adding the glass to the mandrel. I know I made that mistake with my first ever bead. I didn't heat the glass enough and ended up pulling the bead release.

Normally though for me a good soak in water for a bit free's them up. I use pliers, but a pair of old multitool ones there is a convenient circle in them that fits a 2mm mandrel perfectly and holds it tight enough.
Title: Re: Beads are stuck on the mandrels ?
Post by: Glyn Burton on February 05, 2012, 08:50:04 PM
If all else fails I soak them in water and then use my glass grinder. If you have a glastar or similar type of grinder (the sort stained glass artists use) hold the mandrel against the spindle as it is spinning, the flat face on the spindle sets up vibrations which will loosen the bead.
If you don't have a grinder smash it off with a hammer and make another bead, thinking as you do it that practice makes perfect.
Title: Re: Beads are stuck on the mandrels ?
Post by: lampworklover on February 05, 2012, 09:00:13 PM
If you're soaking, hot water will make metal and glass swell up, cold water will make it all contract slightly and might help a bit.
Title: Re: Beads are stuck on the mandrels ?
Post by: Donna@Rockin' Beads on February 05, 2012, 09:33:10 PM
I sometimes put a challenging bead in the freezer for 15 minutes. That can help.
Bead release should be a liquid when it goes on and it dries up in the tub so you do need to add water from time to time.
Good luck.
Title: Re: Beads are stuck on the mandrels ?
Post by: lyzzydee on February 05, 2012, 11:04:18 PM
I have made hundreds of beads and recently I have had three stick, so I have given up with them after trying just about all of the things suggested above!!! The only thing that works with stubborn ones for me is huge pliers and grabbing the bead with damp newspaper.
Title: Re: Beads are stuck on the mandrels ?
Post by: Blue Box Studio on February 05, 2012, 11:23:09 PM
Quote from: Firo on February 05, 2012, 07:31:24 PM
Still laughing at the plant stakes....lol
now wondering if they'd sell...lol

Yes!  Someone wanted to buy one during arts week so I ran round the hopuse, gathered up all the others and sold out.  I make more money from mistakes than I do my good work - which is the fairies trying to tell me something?
Title: Re: Beads are stuck on the mandrels ?
Post by: Glassy Lou on February 05, 2012, 11:37:59 PM
Something I've tried with success is holding the mandrel with pliers just under the bead, then tapping the end closest to the bead with a hammer. You don't touch the bead with the hammer - obviously ;) but the vibration is sometimes enough to shift it. Gently does it.
Title: Re: Beads are stuck on the mandrels ?
Post by: BeadyBugs on February 06, 2012, 08:11:19 AM
I still swear by the Rolson Rivet Gun, or something similar.  There's a thread about it here (http://www.frit-happens.co.uk/forum/index.php?topic=19085.0).  The item link doesn't work any more, but a quick google or ebay search should yield results.  I hope you get them off.   ;D

HP x
Title: Re: Beads are stuck on the mandrels ?
Post by: sarah t on February 06, 2012, 09:21:35 AM
it happens to us all...the dreaded bead release fail  ::)

give the release a good mix/stir /shake ..... i use an old mandrel to get to the bottom and sides and a broken bead in the pot can help mixing it  (lid firmly on or you will join another gang  ;D )

its ok to add water to mix to the right consistancy but try using melted ice/distilled water as the water from your tap may well affect the balance

make sure the mandrels are clean , rinse well to remove any cleaning agent  , i use a green scrubby to give them a key to help the release stick

heat the mandrel and the release along the dip before adding glass

non of the above will stop it happening again (and it will ) but every little helps  ;)


Title: Re: Beads are stuck on the mandrels ?
Post by: Calico Cat on February 06, 2012, 10:53:11 PM
The ones I can't get off - even when the aid of a vice and a rubber glove - I hand over to my OH.

He disappears to his shed with them so I've no idea what he does, but it involves a hammer  ;)

They always come off then but its about 50:50 whether they break in the process.
Title: Re: Beads are stuck on the mandrels ?
Post by: Firo on February 07, 2012, 06:35:52 PM
Tried all of your great suggestions and added my own (a strong man) and saved 3 of the 10 :(, so I'm going to order some new bead release and take your hints on board.....I guess practise makes perfect  ::)
Now I have to find a mail order supplier so any suggestions on best product to use and best supplier gratefully accepted.
Title: Re: Beads are stuck on the mandrels ?
Post by: Madam Steph on February 07, 2012, 06:40:00 PM
Fusion for 'usual' beads and Fosterfire Smooth and Tuff for 'pressed' beads

Linda x
Title: Re: Beads are stuck on the mandrels ?
Post by: Amber on February 07, 2012, 09:12:00 PM
WD40  ;)
Title: Re: Beads are stuck on the mandrels ?
Post by: Jennie Lamb on February 07, 2012, 09:19:42 PM
Try putting them in the Freezer for 24 hours but remeber to use a cloth when you retrieve them....sometimes that helps when all else fails!
Title: Re: Beads are stuck on the mandrels ?
Post by: Donna@Rockin' Beads on February 08, 2012, 07:33:25 AM
I'm more than happy with fusion for all my beads. You just need to make sure the mandrel isn't scruffy before it's dipped.

ETA: I forgot to say that we sell it and I think we have some of the large tubs in stock  :P
http://www.rockinbeads.co.uk/bead/1425-bead-release

10% off if you enter 'FEB12' at the checkout and spend over £20 too
Title: Re: Beads are stuck on the mandrels ?
Post by: Firo on February 08, 2012, 12:26:27 PM
Donna, how much is delivery to Turkey if I spend over £20?
Title: Re: Beads are stuck on the mandrels ?
Post by: Donna@Rockin' Beads on February 08, 2012, 01:17:04 PM
Aha, I hadn't spotted that you wanted it sent to Turkey! It looks like it might be about £4.50.