Has anyone had any experience with these?
I was thinking of getting one but am a little dubious as to whether they would clean out the bead release or not?
I had a jewellery cleaner - small amount of water & it vibrated, but I think it wasn't that brilliant at removing bead release. I have never tried a sonic one.
I have one, it's crap !
Big profesional one and like Sooz said :-\
They work on the grime that collects behind stone settings and remove residue if you have been polishing silver but don't have much impact on bead release - sadly.
Mari
Thanks guys - you just saved me some money - will spend it on more glass!