Lampwork => COE 104 => Topic started by: cbeadies on September 10, 2011, 12:16:20 PM

Title: 'Spreading' glass?
Post by: cbeadies on September 10, 2011, 12:16:20 PM
Hi, I know that rubino and cranberry glasses 'spread' nicely when heated on white glass. Has anyone come across any other transparent colours that do a similar thing? Just wondering! Thanks.  :)
Title: Re: 'Spreading' glass?
Post by: awrylemming on September 10, 2011, 01:01:09 PM
Pineapple and orange sparkle are both spreaders.
Title: Re: 'Spreading' glass?
Post by: cbeadies on September 10, 2011, 01:14:27 PM
 :) thanks Sue, I still have some of the orange sparkle, will try that later.
Title: Re: 'Spreading' glass?
Post by: DellaUK on September 10, 2011, 04:10:20 PM
EDP - Effetre Purple, and inky pen from CIM are have similar effects too.

Della
Title: Re: 'Spreading' glass?
Post by: awrylemming on September 10, 2011, 04:38:19 PM
Mosaic green definitely spreads, but I find it difficult to use as it takes over everything else  :-\