Lampwork => COE 104 => Topic started by: Sheena on August 04, 2011, 10:22:42 AM

Title: silvered ivory
Post by: Sheena on August 04, 2011, 10:22:42 AM
Hello,
I've read alot of people use silvered ivory. Is this something you can buy, or do you have to make your own - and if so how? I've tried using silver foil over ivory but it looks like a big dirty smudge :o not lovely like the pics I've seen here......
Thanks,
Sheena
Title: Re: silvered ivory
Post by: bluefairy on August 04, 2011, 10:33:38 AM
Hello, have you tried silver leaf?  It's a bit thinner and more subtle than foil  :)
Title: Re: silvered ivory
Post by: Lush! on August 04, 2011, 10:35:27 AM
The way I make silvered ivory stringer is warm the top inch of a rod of dark ivory, roll in a strip of silver leaf, burnish on, melt in, melt a large gather and pull a stringer. 

Hope that helps  ;D
Title: Re: silvered ivory
Post by: Shirley on August 04, 2011, 10:37:09 AM
And don't forget you can silver other colours too. Both types of ivory, coral and turquoise just for starters :)
Title: Re: silvered ivory
Post by: noora on August 04, 2011, 11:10:07 AM
It does look smudgy when you've just applied the leaf on the ivory, but when you pull it out as a stringer and put that stringer on something else it turns interesting :)
Title: Re: silvered ivory
Post by: sarah t on August 04, 2011, 11:46:01 AM
if all else fails i have seen silvered ivory stringers for sale on etsy ,but its so easy to do why would you ?

the stringers dont need to be neat or lovely for the effects to work and i find it works best if given a good melt in to make it spread a bit

give it a go  ;)
Title: Re: silvered ivory
Post by: Sheena on August 04, 2011, 02:43:29 PM
Thank-you everyone. I'll try that.  :)
S.
Title: Re: silvered ivory
Post by: Krysia@No98 on August 04, 2011, 04:21:41 PM

make sure you have your extraction going when you do it and that you are not leaning right over it and breathing deeply when you do it, coz you'll really know about it for a good few hours as you wonder if a chest infection is settling in.  ::)

Have fun  ;D
Title: Re: silvered ivory
Post by: Sheena on August 11, 2011, 03:56:44 PM
Hi,
Finally got torch time today and pulled lots of stringers. They worked great! Thanks for all the advice.
Sheena