Frit-Happens !

Lampwork => COE 104 => Topic started by: Lotti on July 30, 2011, 04:18:36 PM

Title: Pale trans green
Post by: Lotti on July 30, 2011, 04:18:36 PM
I have been using Effetre 031 for this but find even this a bit too vibrant, I am looking for something paler than this, any suggestions (without breaking the bank!) ? :)
Title: Re: Pale trans green
Post by: awrylemming on July 30, 2011, 04:27:22 PM
Pale aqua 038 - it's a very delicate colour x
Title: Re: Pale trans green
Post by: SilverGems89 on July 30, 2011, 04:34:36 PM
CIM mojito is lovely, or what about reichenbach antique clear?
Title: Re: Pale trans green
Post by: Lotti on July 30, 2011, 04:40:36 PM
Thanks ladies, I think antique clear is what I was thinking of, but got confused as Martin doesn't seem to have any and I knew it wasn't antique green I wanted.  I already have 038 (well I did, have to order more and love it, but wanted a greenier one, but not too green - if you know what I mean!).  Hopefully Martin will have more in soon, not desperate at the mo! :)
Title: Re: Pale trans green
Post by: SilverGems89 on July 30, 2011, 04:43:17 PM
are you going to Di's Lotti?
Title: Re: Pale trans green
Post by: jammie on July 30, 2011, 04:58:33 PM
Lt emerald is lovely.  :)
Title: Re: Pale trans green
Post by: Lotti on July 30, 2011, 05:21:34 PM
Quote from: jammie on July 30, 2011, 04:58:33 PM
Lt emerald is lovely.  :)

:) :)  I think that's the one I have been using, it is nice and I finished off my first 1/4 of it in no time, just have a hankering for something different. :)

Quote from: SilverGems89 on July 30, 2011, 04:43:17 PM
are you going to Di's Lotti?

Hi, no sadly not, A) long long way away and b) I have a poorly Mummy and have to zip down across the moor again tomorrow to see her.  I wish I was going, looks like a fab day, maybe another time. :)
Title: Re: Pale trans green
Post by: k00m on July 30, 2011, 05:43:50 PM
Effetre Yellow Green (071) looks like it might be a little lighter and isn't actually that yellow from my memory.
Title: Re: Pale trans green
Post by: Shirley on July 30, 2011, 06:41:49 PM
Cim Appletini is nice.

You could also try making a clear core and then encase with your green. That should lighten it a bit.
Title: Re: Pale trans green
Post by: Lotti on July 30, 2011, 06:58:25 PM
Quote from: Shirley on July 30, 2011, 06:41:49 PM
Cim Appletini is nice.

You could also try making a clear core and then encase with your green. That should lighten it a bit.

Funny you should say this, I have just watched Corinna's secret of stringer control and she does encased stringers and I thought, what if...  :)  Might just give it a go! :)
Title: Re: Pale trans green
Post by: Krysia@No98 on July 31, 2011, 01:32:35 PM

What about "Yellow Uranium 591070" which is surprisingly, green or "Pale Apple Green 591073"
Title: Re: Pale trans green
Post by: fionaess on July 31, 2011, 02:42:43 PM
pale apple green is a really pale green