Frit-Happens !

Lampwork => COE 104 => Topic started by: Hazer on July 30, 2011, 03:17:04 PM

Title: CiM Glacier reaction?
Post by: Hazer on July 30, 2011, 03:17:04 PM
Quick reaction question - what is it in CiM Glacier that would react with DH Triton (or vice versa, I guess)? I don't know whether I reduced it too much, but the result was different than expected!
Title: Re: CiM Glacier reaction?
Post by: awrylemming on July 30, 2011, 04:24:07 PM
Did it go pink?  That's the reaction I've had with both that and green tea, although I'm not sure what would cause it.  Copper perhaps?
Title: Re: CiM Glacier reaction?
Post by: Hazer on July 30, 2011, 04:48:00 PM
It went ...ivory coloured. Hang on, got a very bad picture:

(http://farm7.static.flickr.com/6128/5990967038_9cb3f5a75a.jpg) (http://www.flickr.com/photos/continuumdesigns/5990967038/)
weird (http://www.flickr.com/photos/continuumdesigns/5990967038/) by Continuum Designs (http://www.flickr.com/people/continuumdesigns/), on Flickr
Title: Re: CiM Glacier reaction?
Post by: awrylemming on July 30, 2011, 04:56:06 PM
That's really rather lovely.  I don't know why though!  :D
Title: Re: CiM Glacier reaction?
Post by: Lotti on July 30, 2011, 07:04:55 PM
I wondered if it had fumed from the SG, pinks do that alot don't they? :)  I like them too. :)
Title: Re: CiM Glacier reaction?
Post by: shaz on July 30, 2011, 08:01:01 PM
It did exactly the same with me mine looks identical apart from the shape lol