I have tried to make air bubbles with brass shavings but only getting brown spots in the bead. Would anyone mind telling me what I am doing wrong please. ???
Are you using them in boro, as if so it won't work :'( :'( I think the effect only works in soft glass. It's the same with copper, the copper just melts and starts combining with the boro rather than staying intact
I am trying the brass shavings with effetre clear. Do you have to do anything special?
That should be fine, although I've never done that effect myself; there is a link to another thread that might help http://www.frit-happens.co.uk/forum/index.php?topic=15880.0 (http://www.frit-happens.co.uk/forum/index.php?topic=15880.0) :)