Morning peeps
Last time I ordered from DH, I got me some Olympia Rain. All fine and dandy except I haven't a clue what to do with it. I've tried a few beads but they look like bleurgh.
I've seen people achieve some lovely wispy effects with this glass but no idea how
Can someone post me a recipe to try with Olympia Rain, just to get me started?
Thank you
H x
I've never tried it, but I've got a vague recollection that it can be stormed.
Have you tried it as stringer over cobalt?
I have messaged you.
Olympia Rain is marketed as Aion now, a slightly new recipe to iron out the 'shocky', I believe.
You may have bought a 'new' limited edition made by request, which goes back to the original 'recipe', so go easy on the 'warming' at first
Hi Helen
Olympia Rain is great for storming which is why they remade it. Its quite different to Aion although Steph is right that Aion replaced OR a few years ago. I haven't used it other than storming. But you could try it over amber as that usually gives a cool reaction for the transparent silver glasses.
These are OR stormed over an ASK red.
(http://farm3.static.flickr.com/2725/4253893553_275978b5d7.jpg) (http://www.flickr.com/photos/flameforcefive/4253893553/)
Storms over Mars (http://www.flickr.com/photos/flameforcefive/4253893553/) by Flame Force Five (http://www.flickr.com/people/flameforcefive/), on Flickr
Sarah
xxx
This is one of my favourite silver glasses and I use it a lot. It doesn't need a lot of reduction, and I actually prefer it in small amounts over other silver glasses, especially Elektra. I find it very different from Aion, I actually bought a load when I found out it was replacing OR but it's nothing like. Rachel's your woman for this one though. ;)
I was going to suggest the storming tut too, by Amy Kinsch
http://beeswarubberstamps.com/lampworkbeads.htm
I wrote a blog on it aaaages ago....
http://helenjewellery.wordpress.com/2010/10/29/glass-testing-double-helix-olympia-rain/ (http://helenjewellery.wordpress.com/2010/10/29/glass-testing-double-helix-olympia-rain/)
not sure if it will help but have looksie :)
I love those Sarah! x
I was just coming online to say about your blog Helen ;)
Thanks Helen :)
And Sue - I'm itching to try OR with elektra now. Do you have any pictures?
Sarah
xxx
'Fraid not - I've been nagged to death about taking photos and putting a catalogue of sorts together, but I really hate taking pictures. Hence the lack of 'em in the Gallery. I'm going to try more from now on, as once they're sold I have no record of things that I've made, and it would be a rather nice thing to have. The lady who bought the pendant might let me take a piccy if I see her though.
Oh, and it is the best glass for storming. Makes fab twisties and murrini too.
I promise from now on to photo all half decent beads that I make, lampworkers honour ;D
Thanks one and all - I have the storming tutorial so gave it a go on a couple of beads today.
Going in the kiln, they looked a bit birdy poo like but we'll see what comes out!
Helen x
Quote from: awrylemming on July 17, 2011, 04:42:19 PM
I promise from now on to photo all half decent beads that I make, lampworkers honour ;D
We'll hold you to that Sue ;) I like having the photos so that I can see my progress (or lack of it sometimes) and how my style develops.
Helen my stormed OR looked like birdy poo too before it went into the kiln ::)
Sarah
xxx