Frit-Happens !

Lampwork => COE 104 => Topic started by: Ant on July 08, 2011, 08:53:35 AM

Title: CIM Hades
Post by: Ant on July 08, 2011, 08:53:35 AM
I decided to try making a batch of fritty beads on CIM Hades last night and was really disappointed as a lot of the frit seems to have disappeared now they're out of the kiln.  Is it a case of me having over-heated the frit or is it just the reaction of the glass on Hades do you think?  The frit was Beadysam's 'Gem Surprise' which looked like a mixture of white / red / coral / pale blue colours and which I thought would stand out really nicely on the black.

Any suggestions or advice would be really appreciated please before I try another batch of Hades fritty beads!
Title: Re: CIM Hades
Post by: Kaz on July 08, 2011, 09:24:53 AM
Hades is possibly too strong a black - perhaps try eff black instead.
Kazx
Title: Re: CIM Hades
Post by: ARBeads on July 08, 2011, 09:28:12 AM
Hades is like the intense black, pull really thin apply to bead, super heat and you get a lovely lace effect. It's probably 'eaten' the frit.
x
Title: Re: CIM Hades
Post by: Ant on July 08, 2011, 10:18:04 AM
Quote from: ARBeads on July 08, 2011, 09:28:12 AM
Hades is like the intense black, pull really thin apply to bead, super heat and you get a lovely lace effect. It's probably 'eaten' the frit.
x

Yep, it certainly has!  I guess that's how you learn.  I'll try Effetre black with frit then and have a play with hades stringers to see what sort of effects I can get.  So is Hades not really recommended as a base colour then?  I think I saw some beads in the gallery with Hades and Raku frit, which looked really great and that's what inspired me to try the fritty beads.

Thanks for the advice.
Title: Re: CIM Hades
Post by: LilLizaJane on July 08, 2011, 10:36:36 AM
 ::)They were mine! Yes it was Hades base  - raku is strong enough to hold it's own against the 'force of darkness'! These were they:
(http://farm6.static.flickr.com/5038/5888666616_459f3b9cf4.jpg) (http://www.flickr.com/photos/lil-liza-jane/5888666616/)
Raku frit swirled on Hades buttons (http://www.flickr.com/photos/lil-liza-jane/5888666616/) by LilLizaJanes Jewellery Store (http://www.flickr.com/people/lil-liza-jane/), on Flickr
Bethx
Title: Re: CIM Hades
Post by: jammie on July 08, 2011, 10:47:41 AM
Pretty, that's a nice press shape too.
Title: Re: CIM Hades
Post by: LilLizaJane on July 08, 2011, 12:01:26 PM
Thank you! It's a Bavarian one - 'button trio'.
Title: Re: CIM Hades
Post by: Lush! on July 08, 2011, 01:08:26 PM
Ant, why don't you try encasing a TINY Hades bead then add your frit to the clear surface?  (I know you make great encased beads  ;))
Title: Re: CIM Hades
Post by: Kalorlo on July 08, 2011, 11:53:04 PM
Gem Surprise has some transparents in it as well as the opaques - they won't show up on the black so I'd agree with what Julie said to try.

Though... hades with silver leaf and *then* the frit could be nice.
Title: Re: CIM Hades
Post by: Ant on July 09, 2011, 11:15:58 AM
Thank you all - back to the torch it is then!  ;D