Frit-Happens !

Lampwork => COE 104 => Topic started by: Fruddy on June 22, 2011, 03:55:22 PM

Title: Belladonna Glass has finally arrived.....
Post by: Fruddy on June 22, 2011, 03:55:22 PM
.... and I am going to go and have a play with it, to see what I can produce.

Got two colours, Moody Blue and Purplescent.... the website states that best results are produced using a Dragon's Breath reduction flame, never done this before, so that'll be interesting, if nothing else!

Will post some photos if I manage to produce anything half decent!
Title: Re: Belladonna Glass has finally arrived.....
Post by: awrylemming on June 22, 2011, 03:56:52 PM
I read about the Dragon's Breath flame too - I'll be interested to hear how this goes  :)
Title: Re: Belladonna Glass has finally arrived.....
Post by: flowerjasper on June 22, 2011, 06:09:26 PM
look forward to the pictures  ;)
Title: Re: Belladonna Glass has finally arrived.....
Post by: Jennie Lamb on June 22, 2011, 08:40:53 PM
Great!  Looking forward to seeing the pics!!
Title: Re: Belladonna Glass has finally arrived.....
Post by: Princess Peggy (Priscilla McGirr) on June 23, 2011, 03:26:08 PM
Me too!