Why did my rod of mermaid half way through using it develop spots of poo? I was not impressed :-X
So was it me or was it the glass?
:) Thank you Oh Wise Ones
I had the same thing, but it was because I was working it too hot. I ended up with little brown 'scorch' marks. I now work it towards the end of the flame, and it doesn't happen any more.
This could be it. I was making 2 on the same mandrel and it was always the first one that did it. Thinking back it was when I went back to give it some extra heat so it didn't get too cool.
Lesson learned :)
Thank you Sue :0 xx