Post by: SilverGems89 on May 17, 2011, 11:34:15 AM
Ok i've been waiting for ages to get some EDP and had loads of ideas what to do with it, well the post man just kindly bought me some EDP and guess what? my mind has gone blank....what was i going to do with this stuff again? I've tried a search of the forum but didn't come up with much, so anyone got any tips on what to do with it? pleeeeeeeease?  ;D
Title: Re: EDP
Post by: helenfc on May 17, 2011, 11:39:28 AM
Try it on a dotty bead gems, its spreads like rubino :)
base of copper green or opal yellow, edp dots and then periwinkle or new violet or some other opaque on top. Tis yummy! Have fun! xxx
Title: Re: EDP
Post by: SilverGems89 on May 17, 2011, 02:16:24 PM
well i say! move over rubino oro, you may just have been replaced in my favourites category  ;D
Title: Re: EDP
Post by: GlassOcean on May 17, 2011, 02:17:18 PM
Try fuming an ivory bead with it, comes out all matt and interesting!
Title: Re: EDP
Post by: Hotglass28 on May 17, 2011, 07:20:12 PM

Stick it in the flame and have a play. Only way to go  ;)
Title: Re: EDP
Post by: Donna@Rockin' Beads on May 17, 2011, 07:47:10 PM
Just use it as normal combined with lime green. Fab.
Title: Re: EDP
Post by: flowerjasper on May 17, 2011, 08:15:52 PM
it is a naughty one, if it devits, just heat up again,
i pull stingers and use it on dottie beads, its is great with dirty martini, torquoise, violets, pale pink green,
have a play  ;)
sandy
Title: Re: EDP
Post by: suzielaws on May 17, 2011, 09:50:39 PM
It is lovely in twisties as well and looks yummy when etched, I use it a lot to make owls. Dont forget to post your pictures.
Title: Re: EDP
Post by: Justmade on June 01, 2011, 06:51:00 PM
If you want your EDP to turn a fab fuchsia purple, make your bead, take it out of the flame and blow on it! The quick cooling of your EDP will make the color pop. If you find your bead has devit on it, reheat it in the flame untill it becomes shiney again, and then... blow. For real :)
Title: Re: EDP
Post by: Brink Beads on July 05, 2011, 12:58:59 PM
Gonna try the blowing thing  ;) sounds like it will produce just the colour i'm looking for.

Thanks Justmade xxx
Title: Re: EDP
Post by: LilLizaJane on July 08, 2011, 10:39:07 AM
Could someone tell me the catalogue number of EDP? I get it mixed with ordinary Effetre purple!
Title: Re: EDP
Post by: SilverGems89 on July 08, 2011, 11:09:46 AM
Effetre 254  ;D
Title: Re: EDP
Post by: LilLizaJane on July 08, 2011, 12:02:23 PM
Thank you. Noted and labels changed!
Title: Re: EDP
Post by: SilverGems89 on July 08, 2011, 12:07:00 PM
It's a lot more of a pinky purple than the standard effetre 272 purple so they're fairly simple to tell apart if you ever get them mixed up!