Last week I made a beautiful set of beads for a commission. Etched them and now they look pants! Yesterday time to redo them. This time the silver wire round the middle has fumed EVERY one of them!!! Why :-[ :-[ :-[ :-[ It didnt do this with the first set. The glass is the same, the wire is the same. Lots of time and money wasted so far, not to mention my self esteem :(
No idea but would love to know - I've had the same problem recently! I put it down to my getting things too hot or too near the torch head on my HH.
I think it's probably your flame - try turning up the oxygen a bit.
Quote from: Lush! on May 05, 2011, 08:04:11 AM
I think it's probably your flame - try turning up the oxygen a bit.
As Julie says (and she should know!!! :D)
the worst thing is that they are for a colleague of my husbands, who has the potential to be a very good customer...and now im panicking :-\ :-\ so website stuff this morning will have to wait...will go try again :'(
Sorry for my curt response earlier, I was on my phone in bed!
Good luck with trying again Sarah - what colour glass is being affected? I find any pinks, white and periwinkle are the worst offenders. Just turn up your oxy a bit so that you're definitely not reducing, an extra whiff of propane is all that's needed to cause the problem.
Quote from: Lush! on May 05, 2011, 08:39:42 AM
Sorry for my curt response earlier, I was on my phone in bed!
Good luck with trying again Sarah - what colour glass is being affected? I find any pinks, white and periwinkle are the worst offenders. Just turn up your oxy a bit so that you're definitely not reducing, an extra whiff of propane is all that's needed to cause the problem.
I didn't think your response was curt :)
Its CIM Tuxedo, Effetre steel grey and dark purple. The tuxedo ones look lovely if you want blackie blue beads...which Julianna has already claimed :)
I don't use Tuxedo - you could try Effetre Black instead?
hi jacking slightly ...is there a white that does not fume as much ?...i am trying to make white with aurea and to get the effect from one you fume the other :(
Defo to do with the flame Sarah as Julie says :0
Quote from: Lush! on May 05, 2011, 08:52:39 AM
I don't use Tuxedo - you could try Effetre Black instead?
I only have tuxedo...and they WILL be done today :)
Quote from: sarah t on May 05, 2011, 08:53:17 AM
hi jacking slightly ...is there a white that does not fume as much ?...i am trying to make white with aurea and to get the effect from one you fume the other :(
The ONLY white I have found that doesn't fume
as much (as long as you treat it very carefully, turn up the oxy) is P&T Diopal White. Unfortunately its not 104 (they make glass with 2 COEs and I can't remember which this is) so its not compatible with DH, although you may get away with a tiny bit - but the white will probably get fumed anyway when you reduce the Aurae. I'll try to remember to have a go for you.
I only use it for my Sunbaked Beads when its just plain white with silver round.
thanks julie :-*
Quote from: Lush! on May 05, 2011, 08:04:11 AM
I think it's probably your flame - try turning up the oxygen a bit.
Another reason why I really really do need a big girl's torch then [as if I need any more reasons to justify]! Hard to get more oxygen on a HH, and I'd already tried turning the gas down.
Hmmm, would working a bit higher help, Sue?
Quote from: Lush! on May 05, 2011, 09:22:04 AM
Hmmm, would working a bit higher help, Sue?
I think my chair is as high as it will go Julie
[sculks off before the rotton tomato lands....]
I'm trying to justify buying a new torch and oxycon to hubby, don't blow my cover
;D ;D ;D
;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D
NON fumed black and purple beads in kiln...oxy up and job's a good 'un
(had to rush to dr's to pick up inhalers for the idiot with asthma who let them run out and needed them like yesterday and surgery is only open 2 hours a day)
...now off to redo the grey ones :) :) :) :) :)
THANKYOU XXXXXXXXXXXXXXXXXX
Oh fantastic! I'm so pleased, Sarah!
yay, result!! :)
Quote from: The Tartan Trout on May 05, 2011, 07:35:29 AM
This time the silver wire round the middle has fumed EVERY one of them!!!
Sarah, what does this mean, please?
Linda, it means that fumes from the silver, released in the flame, have affected the glass. This can often be a good thing which we would do on purpose for organic effect, but its very often a bad thing when you just want a nice clean shiny bead with nice clean shiny silver decoration.
I think the fuming effect turned Sarah's black glass a kind of smoky blue. It can turn white or pink (etc) a nasty yellow brown. But it can also turn white a fab rich toffee brown if you want it to!
Thanks, Julie.
I can guess that much the same thing can happen with a Hot Head, so this will go into my file labelled "Tips to Prevent Pitfalls".
I know how Sue feels about wanting a big girl's torch. That Cricket I tried at Flame Off was so much faster than my Hothead, but it's only a week, and I'm getting better at shaping and it's giving me a good grounding, I daresay, for when I can afford to 'step up' to a faster torch. The thing I'm impatient about is not being able to use the silver glasses, but then there are lots of nice glasses to be getting on with, and when my special glass arrives (I HAVE ordered some) then I will mess about with the foil/glove.
I can't see waiting long though ::)