Frit-Happens !

Lampwork => Common Problems => Topic started by: The Tartan Trout on April 28, 2011, 09:26:36 AM

Title: partially etched beads :/
Post by: The Tartan Trout on April 28, 2011, 09:26:36 AM
I have just taken the loveliest set of beads out the kiln...steel grey, dark purple and tuxedo black...all with wire wrapped round. Happy dance commences :) The person that requested these beads also wanted them etched...now they are minging and nasty :( The black has only etched round the middle on all of them. I tried redoing them and the results were the same.
Is it the glass or is it me? So cross  >:( as now I have to redo the whole bloomin lot!!! 
Title: Re: partially etched beads :/
Post by: sparrow on April 28, 2011, 09:30:23 AM
Some glass doesn't etch (Terra is a famous one) - sounds like you've got either a glass or a reaction in there that doesn't etch - if you want, you can send them to me and I can try sandblasting them - no guarantee it'll work, but if they're not fit for purpose anyway.....?  :-\
Title: Re: partially etched beads :/
Post by: paintboxcrafts on April 28, 2011, 10:11:31 AM
I have found that Cim Tuxedo, Halong bay and Poison apple do not etch.
Cathy
Title: Re: partially etched beads :/
Post by: The Tartan Trout on April 28, 2011, 03:49:21 PM
Thanks Sabine, but I will put them into the 'lesson learned' box.
Cathy it was CIM Tuxedo Black. I won't make that mistake again

x
Title: Re: partially etched beads :/
Post by: Magpie on April 28, 2011, 04:06:16 PM
Bacardi bottle beads may or may not etch depending on whether they're in a mood of not. I had two which got dunked in the etching fluid at the same time for the same time, one etched, one didn't!