Frit-Happens !

Lampwork => Common Problems => Topic started by: Amber on April 27, 2011, 12:44:43 PM

Title: What's going on here then?
Post by: Amber on April 27, 2011, 12:44:43 PM
(http://i171.photobucket.com/albums/u286/Spookyjewel/024-1.jpg)

Loads of my etched beads have developed this white gunk around the bead holes and I'm really worried about the ones I've sold now... :-\

What is it and can I get rid of it?
Title: Re: What's going on here then?
Post by: ARBeads on April 27, 2011, 01:08:02 PM
Not seen that before, are you remembering to neutralise the etching fluid in a solution of Bicarb/water and then a really good rinse in plain water?

Just a thought x
Title: Re: What's going on here then?
Post by: Josephine on April 27, 2011, 01:10:36 PM
I agree, neutralise and then give them a gentle scrub with an old toothbrush and a tiny bit of washing up liquid in warm water.
Title: Re: What's going on here then?
Post by: Les on April 27, 2011, 01:13:40 PM
I use an old toothbrush too. It works a treat :)
Title: Re: What's going on here then?
Post by: ScarletLeonard on April 27, 2011, 02:48:04 PM
ahhh bicarb and water.... thats what I was doing wrong, I get that gunk around the dots.
Title: Re: What's going on here then?
Post by: Magpie on April 27, 2011, 10:38:54 PM
Quote from: Josephine on April 27, 2011, 01:10:36 PM
..... a gentle scrub with an old toothbrush ......
Quote from: Lesley Jane on April 27, 2011, 01:13:40 PM
I use an old toothbrush too.

So was it wrong to use D's toothbrush? He hadn't done anything to annoy me, but there were only two toothbrushes and there was no way I'd use mine! Should I have used toothpaste to scrub with or was the soap OK? He didn't say it tasted funny or anything......

::)