Frit-Happens !

Lampwork => Common Problems => Topic started by: Passionatelamper on April 22, 2011, 03:35:08 PM

Title: Torch
Post by: Passionatelamper on April 22, 2011, 03:35:08 PM
Hi there can someone please help me!!  :-\
I am having problems with the torch... I have this white sort of flame about half inch deep that wont go.
I have cleaned out the nozzles of the torch with my pokey tool but it still wont go.
I did melt some glass in the week and I think some landed in the torch head but not sure.
I think I must be coming to the end of the propane as well as I have to keep turning up the gazzzz :)
Perhaps some hot head out there lols can lead me the way lols.
Thank you :)
Is there a tool you can get that tells you how much propane you have left?
Only I cannot possible run out...oh nononnonoo no.
ha- ;D ha!
Title: Re: Torch
Post by: Mand on April 22, 2011, 03:43:33 PM
I have a solution but you won't like it !   :o-- Throw it away and buy a Minor!  ;) :-*  Sorry that's not much help, I never did get on with my HH.  I hope someone can help you very soon.  ;)
Title: Re: Torch
Post by: Veebee on April 22, 2011, 03:44:46 PM
Is your gas on full? I fully open the gas, fully open the regulator then turn back a quarter turn (you turn the regulator the opposite way to turning on the gas to open it) when the torch is lit turn it up full. Should be fine unless, as you say, you are out of gas!
Title: Re: Torch
Post by: Alison G on April 22, 2011, 04:27:53 PM
Clean easy, and yes I know it's not spelt that way, but I can't bear the butchery, sell a stick on indicator. I have one but my tank is full so it's not dropping yet.

Don't throw the HH  :) if there is glass it in you could try something that worked a treat on my minor, I don't see why it wouldn't on a HH.

I was suggested a couple of ways. Undo it from the clamp turn it upside down and give it some sharp taps then try the poky thingie, but be careful not to break it in the jets. That didn't work for me as mine was pretty blocked so I tried method two.

Unclamp the torch but make sure it's propped up and supported properly, we left the bracket on and just unscrewed it from the bench. Let it get properly hot and then turn off the gas, before plunging it into cold water. That shocked most of the glass out of mine. Hub had to do it a couple of times though.

It still pushed little bits out for a few days but I'd lost that long, white flame you mention.

Someone else suggested (Sally Carver I think :):) getting someone with a compressor, like a garage or workshop, to hook it up and give it a good blast of air.

I hope you can fix it, it's so frustrating isn't it?
Title: Re: Torch
Post by: Blue Box Studio on April 22, 2011, 04:30:55 PM
Quote from: Alison G on April 22, 2011, 04:27:53 PM
Clean easy, and yes I know it's not spelt that way, but I can't bear the butchery, sell a stick on indicator. I have one but my tank is full so it's not dropping yet.


Not very reliable, I sent mine back!  Doesn't fit on the 3kg cylinders either (not that I have one now).
Title: Re: Torch
Post by: ScarletLeonard on April 22, 2011, 04:32:26 PM
I can help with the gas indicator

Caravan shops sell these little plastic things that you stick on to the gas bottle and it gives you a rough indication of the levels.
stick it near the bottom of the bottle and when the gas reaches the strip it will show up.
They are reuseable.

Cross posted with Alison there...

As for the white flame, no idea
When your torch is really cold make a loose fist around the top of the nozzle then blow really hard into your hand, you should then hear if there is anything rattling about inside the head.

ignore those people telling you to chuck it out and buy a duel.... :p
Title: Re: Torch
Post by: jammie on April 22, 2011, 04:33:56 PM
I have had problems with mine too. To clean it you can knock it  and do the air thing. Last resort is to unscrew it and take out the little bit inside and prick it with a pin. This worked for me. I can find a bit for you online that shows you a diagram  if you like.
Title: Re: Torch
Post by: MadelineBunyan on April 22, 2011, 04:35:59 PM
just cause you and the cricket didn't get on Scarlet!

I heard the gas indicators were rubbish. I weigh mine. not the easiest thing to do though. plus you need to know an empty weight of the tank.
Title: Re: Torch
Post by: Blue Box Studio on April 22, 2011, 04:38:17 PM
Apparently the empty and full weight are on the silver collar but darn if I can understand all those stamped numbers.  No doubt there's something on a calor site somewhere.
Title: Re: Torch
Post by: ScarletLeonard on April 22, 2011, 04:40:05 PM
they are a bit poop but it can give you a rough idea at least.

thats one thing the little cans of mapp had going for them, they formed a nice icey layer on the outside when they were running out. I do try and gauge mine by how cold the cylinder is though. Occasionally I grab the top and give it a shake to see what I can hear.

See I am highly technical :p

Quote from: MadelineBunyan on April 22, 2011, 04:35:59 PM
just cause you and the cricket didn't get on Scarlet!
exactly.... evil little blighter.
Title: Re: Torch
Post by: Helen G on April 22, 2011, 04:58:46 PM
I've never done this myself but apparently it can work and it sounds like you do have some glass stuck in the somewhere.

1 Light the torch for a minute so the end is nice and hot.

2 Turn if off and immediately plunge the end face down into cold water.

The idea being you shock the glass out of the torch  ;)
Title: Re: Torch
Post by: jammie on April 22, 2011, 04:59:28 PM
I do the shake thing. Mine always runs out in about 2 -3 weeks so it is possible to have an idea when it will go. I have noticed though that it is sudden when it does finish, the smell and the low heat and there is a point where the pressure just seems to drop and I get further and further towards the torch. By then its usually a weekend and the place to get it is shut! But mine ran out yesterday so I got new today so haha to my propane tank trying to catch me out this time.  :)
Title: Re: Torch
Post by: Passionatelamper on April 22, 2011, 05:26:15 PM
Ok Guys thank you so much  ;D
I actually don't have a hot head it's a Nortel Minor.
Sorry If I mislead you.
It's kinda screwed down.
BUT thank you all for your help  :-*
Title: Re: Torch
Post by: Alison G on April 23, 2011, 09:19:07 PM
Mine was too, but if you unattached it from the bench but keep it on the bracket, that's what I did. The water plunge worked a treat too.

Love my minor!