Post by: helbels on April 13, 2011, 06:34:54 PM
Hiya

I'm periodically tempted by buying a bead liner, but to be honest, all this talk of having to anneal silver tubing puts me right off.  I have a tiny work area, and no real room to store lots of tools etc, and it all sounds a bit of a pallaver tbh.

Anyone want to persuade me otherwise?
Title: Re: How much of a faff is annealing silver?
Post by: MangoBeads on April 13, 2011, 06:37:07 PM
It's no problem you only need a small torch and a cup of water takes seconds , don't let that put you off !
Title: Re: How much of a faff is annealing silver?
Post by: helenfc on April 13, 2011, 06:48:17 PM
Its fine, doesnt take long at all, you could just get a wee kitchen creme brulee type torch for it, they are cheap and easy to refill :)
Title: Re: How much of a faff is annealing silver?
Post by: Redhotsal on April 13, 2011, 06:53:24 PM
Well, yes, I agree with the above - but you'll also have to pickle your silver too because when you heat it up it'll go black. You can get safety pickle from Cooksons etc. or I used to pickle mine in slightly warm Cilit Bang, which seemed to work quite well.
Title: Re: How much of a faff is annealing silver?
Post by: turnedlight on April 13, 2011, 07:01:53 PM
Ooh, good tip - I am just about out of my pickle from cooksons! ;D
Title: Re: How much of a faff is annealing silver?
Post by: Kaz on April 13, 2011, 07:24:09 PM
I buy the pre-annealed stuff from Ginko or the thin wall from rashbels and do no annealing or pickling at all!
Kazx
Title: Re: How much of a faff is annealing silver?
Post by: noora on April 13, 2011, 08:37:37 PM
If you have a kiln you can anneal silver in the kiln :-) The annealing temperature of sterling silver is between 600-650 C and you only have to heat it for a few minutes. I find kiln annealing of silver to be much easier than annealing with a torch, since you don't risk overdoing it and melting the silver.

You still have to pickle it to remove the tarnish and most likely brush/polish it as silver often goes a bit matte when you heat it.
Title: Re: How much of a faff is annealing silver?
Post by: Blue Box Studio on May 20, 2011, 07:11:21 PM
Quote from: MangoBeads on April 13, 2011, 06:37:07 PM
It's no problem you only need a small torch and a cup of water takes seconds , don't let that put you off !

You need a soft cushion on the floor to kneel on as well - or isn't hiding under a cupboard a necessary part?  ;)  ;)  ;)
Title: Re: How much of a faff is annealing silver?
Post by: MangoBeads on May 20, 2011, 09:38:26 PM
ofcourse ! ;D