As I have said previously I am new at this, I have made a bead out of silver black which looked ok as I was melting it, the resulting bead is awful, dull feels like a ceramic pot. I am guessing that I did something wrong. I am on a hothead and my educated guess is that I have over cooked it and taken all the shine away. Should I just be using it as shiny dots ?
Do you have any suggestions???
Pretty much what I get - does it do anything else? Rachel gave a load away because she didn't like it, and can't say as I'm a fan :-\
Aw thats disappointing, I had big ideas for it. I wonder how you get anything decent out of it??
i think Julie lush blogged about silver black...will see if i can find it!
hmmmm must have been imagining it, but i know that silver black very rarely stays "shiny" it usually goes matt and sometimes has a "crinkly" appearance, it is really lovely used in the right way!
Somebody else will be able to give you a much better idea what to do with it - I'm sure loads of people have done wonderful things with this glass. Just not me! ;D
ah ha found this thread about it http://www.frit-happens.co.uk/forum/index.php?topic=17504.0
In my head it was going to be a shiny silver substitute so that I could add very arty spots of silver black on my perfectly formed beads (NOT!!!)
Still I am sure one day it will come in useful when someone commissions me to make a bead that looks like a tar mac road surface!!!
it's beautiful - I love it, it's like lava ;D
I have read the linked thread and I will give it another go tomorrow, I fancy getting the peacock colours (says she like she knows what she is talking about!!!!) I think I over did it today, I will try the letting it cool trick and see how that goes, I am on a hot head so we'll see.
Thank you
I love silver black, I find it looks like leather :)
For shiny black I would go for CIM gunmetal though, if you would like to swap some silver black for gunmetal lizzy then let me know :) x
I'm sure I read somewhere that it's a good base for a silver glass - or perhaps that was the gunmetal. Might be worth doing a search?
Quote from: SilverGems89 on March 26, 2011, 09:59:32 PM
i think Julie lush blogged about silver black...will see if i can find it!
Love silver black - shiny one minute, elephant hide the next. Just use it, abuse it and love it for what it is ;D
I love it too, got some great colours out of it, but it was a bit rough round the holes. :)
Another fan here ;) It's fantastic for 'man beads'...