Frit-Happens !

Lampwork => Common Problems => Topic started by: Veebee on March 23, 2011, 02:06:13 PM

Title: Best bead release for presses?
Post by: Veebee on March 23, 2011, 02:06:13 PM
Wot it said  :)

Those of you who use presses will know this situation, especially if it's a tricksy press that requires multiple pressing.... You make a bead, press a couple of times then the release cracks on you preventing further working. So what's the answer please? Which is the best release for using with presses?
I'v found blue Sludge to be much tougher than Fusion Plus, but Martin seems to have stopped selling it (it was only in the small pots but these seem to be fusion as well now?  :()

So do you have a favourite, and, where do you get it from?

Thanks!
;D
Title: Re: Best bead release for presses?
Post by: julieHB on March 23, 2011, 02:13:40 PM
Manda sells Fusion Plus, which is very good: http://www.mangobeads.co.uk/index.php?page=shop.product_details&flypage=flypage.tpl&product_id=20&category_id=27&option=com_virtuemart&Itemid=1
Title: Re: Best bead release for presses?
Post by: JaySpangles on March 23, 2011, 02:13:55 PM
I use fusion - simply because I get it from Martin along with my other stuff, I just adjust the size of mandrel according to the press I am using.  (Generally for Zooziis I use 1.6, but 2mm is ok for Bavarian Beads and Beadpress.  Don't know about any others.
Title: Re: Best bead release for presses?
Post by: JKC on March 23, 2011, 02:14:28 PM
Do you let go of the mandrel when pressing?   I find that helps.
Title: Re: Best bead release for presses?
Post by: Veebee on March 23, 2011, 02:55:02 PM
Quote from: JKC on March 23, 2011, 02:14:28 PM
Do you let go of the mandrel when pressing?   I find that helps.

Yes, I do.  :)

Thank you guys

I have Fusion Plus Julie, we get along fine for regular beads but have a hate hate relationship with the press. I might have a go with a thinner mandrel though.

I've heard mention of Fosterfire elsewhere, anyone know if it's good for presses?
Title: Re: Best bead release for presses?
Post by: JKC on March 23, 2011, 02:56:50 PM
I just use Fusion, tried Fusion plus, doesn't work at all for me.
Title: Re: Best bead release for presses?
Post by: Blue Box Studio on March 23, 2011, 03:29:45 PM
Quote from: JKC on March 23, 2011, 02:56:50 PM
I just use Fusion, tried Fusion plus, doesn't work at all for me.

I didn't get on with it either.  I just assumed chipping the bead release on a press wa one of life's little challenges.
Title: Re: Best bead release for presses?
Post by: mizgeorge on March 23, 2011, 03:33:33 PM
Fosterfire ;) Much tougher to break!!
Title: Re: Best bead release for presses?
Post by: ♥♥Tan♥♥ on March 23, 2011, 03:36:07 PM
Fosterfire from me too, I get it here

http://cgi.ebay.co.uk/FOSTERFIRE-Bead-Making-Release-Large-16oz-HEAVY-DUTY-/190409113133

Brilliant stuff, it takes a heck of a hammering
Title: Re: Best bead release for presses?
Post by: Blue Box Studio on March 23, 2011, 03:39:09 PM
Heavy duty, smooth & tough, or regular?

[and yes, I am asking in the right thread!]  ::)
Title: Re: Best bead release for presses?
Post by: ♥♥Tan♥♥ on March 23, 2011, 03:39:55 PM
 ;D ;D

I have used all of them and get pretty much the same results
Title: Re: Best bead release for presses?
Post by: Veebee on March 23, 2011, 03:40:59 PM
I just found that Bead shed listing with a search on google which came up with the FH supplier thread, how cool is that?!  ;D
Thank you all!
:-*
Title: Re: Best bead release for presses?
Post by: mizgeorge on March 23, 2011, 03:46:24 PM
I like smooth and tuff, but I agree, the results are just as good with all of them.
Title: Re: Best bead release for presses?
Post by: Shirley on March 23, 2011, 03:47:02 PM
I use FF regular. Wonderful stuff.
Title: Re: Best bead release for presses?
Post by: Les on March 23, 2011, 03:56:54 PM
Quote from: mizgeorge on March 23, 2011, 03:33:33 PM
Fosterfire ;) Much tougher to break!!

And I am one rough mamma when I am beading ;D
Title: Re: Best bead release for presses?
Post by: julieHB on March 23, 2011, 04:02:13 PM
I cannot remember for the life of me who said it, but I am sure I have been told that, whichever bead release you use, it is important to keep the bead release warm for it to keep sticking to the mandrel and not breaking after it has initially been warmed up. This may be the reason why people have problems with cracking when using presses and when making long beads. Just a thought... :)
Title: Re: Best bead release for presses?
Post by: Veebee on March 23, 2011, 04:04:08 PM
Hmm, I do always get it straight back in the flame after pressing, but I will bear that in mind, thanks Julie  :)
Title: Re: Best bead release for presses?
Post by: Kaz on March 23, 2011, 04:12:52 PM
I have had more problems with this last batch of fusion than I have had previously. I thought it was just me as it has been stored in the shedio for quite a while. I am having real problems with the BHBs in rollers.
Kazx
Title: Re: Best bead release for presses?
Post by: hollergrafik on March 23, 2011, 04:48:45 PM
Foster Fire regular for me, stays put on the mandrel but equally easy to get the beads off after.
Title: Re: Best bead release for presses?
Post by: Veebee on March 23, 2011, 04:54:59 PM
Thank you all very much! I have ordered some fosterfire for when I'm pressing or generally being thoroughly abusive to the beads in question. I'll keep the fusion for more normal beads  ;D

Ah Kaz, no it's not just you hun  ;)
Title: Re: Best bead release for presses?
Post by: JKC on March 23, 2011, 07:20:50 PM
http://cgi.ebay.co.uk/FOSTERFIRE-Bead-Making-Release-Large-16oz-HEAVY-DUTY-/190409113133   - must have been a rush on - none left.
Title: Re: Best bead release for presses?
Post by: Shirl on March 31, 2011, 10:55:32 PM
I would like to get some Fosterfire as well, does anyone know of any suppliers that have it in stock?
Title: Re: Best bead release for presses?
Post by: Alison G on April 21, 2011, 09:18:18 PM
Bit late to the party but I have tried pretty much all of them, I like the Foster Fire but I think it's a pig to clean, it worries me as I have lung problems.

But at FO I found the best release ever! It's by Christina at Frit en Glas. You really have to get it hot to make the glass stick initially, but once you have it doesn't move. I have never had to use pliers to remove a bead and I don't soak them. I just clean outside now, it's much less dusty IMO because you can use a super thin layer.

I'm a convert!
Title: Re: Best bead release for presses?
Post by: MadelineBunyan on April 22, 2011, 09:16:28 AM
Im not a presser, cant get on with the things, when I had one I did find fusion cracked.

I also find it cracks doing bhbs in rollers, but I think this is because of what Julie hb said about the bead release being cooler, one the last few beads that cracked, I've been noticing it more and more, the bead release definitely got too cold.

dusty Alison? are you not taking the beads off wet? even if they don't need soaking they should still be wet.

I will try some of Christina's bead release soon, but I wont be able to tell you what its like for pressing, cause I only have charmbox and I never use the bottom half anymore
Title: Re: Best bead release for presses?
Post by: GaysieMay on April 22, 2011, 10:25:18 AM
I always heat the mandrel right next to the bead hole at both sides before pressing and I do think this helps.
Title: Re: Best bead release for presses?
Post by: Alison G on April 22, 2011, 11:51:46 PM
Quote from: MadelineBunyan on April 22, 2011, 09:16:28 AM
Im not a presser, cant get on with the things, when I had one I did find fusion cracked.

I also find it cracks doing bhbs in rollers, but I think this is because of what Julie hb said about the bead release being cooler, one the last few beads that cracked, I've been noticing it more and more, the bead release definitely got too cold.

dusty Alison? are you not taking the beads off wet? even if they don't need soaking they should still be wet.

I will try some of Christina's bead release soon, but I wont be able to tell you what its like for pressing, cause I only have charmbox and I never use the bottom half anymore

I take them off inside a towel, I am really wary of the dust because I have chest problems, but no not wet.

Do you think I should?
Title: Re: Best bead release for presses?
Post by: Shirl on April 23, 2011, 12:04:30 AM
YES.....do it wet. Then there is no dust, the dust is bad for you.

I dremmel mine underwater too.....get them nice and clean before using them.
Title: Re: Best bead release for presses?
Post by: MadelineBunyan on April 23, 2011, 07:53:43 AM
I have to say it did concern me a tad at FO, all these people happily pulling beads off dry, then buying kits and thinking its ok to do that when they're at home, making loads of beads.

I find that mine come off much easier, even just being dipped in water, also, I use the mandrel to clean out most of the bead release (which is easy to do wet) before I go near it with a diamond bit (diamond bits don't actually like bead release, particularly fusion, wears them out poor things)

drilling glass (which is essentially what you're doing when you are dremelling beads) is done wet for a number of reasons, cooling being one of them, and making the diamond bits last longer (presumably this is linked to the keeping it cool it thing). as well as this you've now not only got bead release dust flying around, but glass particles and anything that wears off the diamond bit.
Title: Re: Best bead release for presses?
Post by: sarah t on April 23, 2011, 10:36:55 AM
alison ..naughty naughty  ;D
soak em ,clean em ,ream em ..under water ....thats the beads and mandrels not you  :P ...and sal says dont tip the realease cleaning water down the sink ....but so much crap goes down my sink i think thats the least of my worries  ;D...famous last words ???

i did not think much to the christina release...thats not to say it aint good just did not work for me  ......maybe i did not get it hot enough ???......and it dries the same colour as the mandrel so i could not see it  :(........i had a bead stick on the mandrel which has not happened for yonks ......i would rather it went before i finished the bead ..not being able to get it off the mandrel is just not playing fair  :D......think i will stick to my forest fire ....
Title: Re: Best bead release for presses?
Post by: awrylemming on April 23, 2011, 12:53:34 PM
You clean them dry?!!  Scary lady, get them in a pot of water, clean them, drain off the water, scrape damp release into bin with kitchen roll, safer innit!
I must say, I loved Christina's release too.  My beads came off the mandrel much more easily, especially the pressed ones, and it was incredibly simple to clean my beads afterwards.  I just wish it was easier to buy ...
Title: Re: Best bead release for presses?
Post by: jammie on April 23, 2011, 12:58:40 PM
I like Manda's fusion plus. Did think of trying the fosterfire but dont think Sooz id doing any lampwork stuff now?
Title: Re: Best bead release for presses?
Post by: Alison G on April 23, 2011, 09:20:32 PM
I promise to be good from now on, ladies :)