I am a novice bead maker, had a couple of courses and I have a good book, so far I have concentrated on trying to make a decent shape bead, which I think I have (specialising in donut beads!!) I haven't had a bead stuck on the mandrel and only one breakage out of about 100 beads, so on balance I think I am doing well.
On the negative side I am struggling with making two beads the same, (size or pattern or effect) I think perhaps I am too impatient wanting to do everything at once and falling short.
I have made some nice spotty sputnik types, a couple of stripey ones and they have a whole box of odds and sods!!
So what would you suggest I try that gives a good (or spectacular!!) result and will bolster my confidence ?
I find tornado beads always make me feel better - they look far more complex than they are, and are extremely satisfying to do.
Gravity Beads - Really easy and they don't have to be a perfect match.
have you got any bead presses or rollers ? they are good for doing the same .........well as the same as i can get them !
What is a tornado bead? Are gravity beads what I am already doing?? (Making a disc and melting it down?)
Quote from: lyzzydee on March 20, 2011, 05:36:23 PM
What is a tornado bead? Are gravity beads what I am already doing?? (Making a disc and melting it down?)
Gravity beads .. make bead, add a second colour, melt in, let the whole thing droop a bit and turn the mandrel, drrop a bit more and turn again, until you get a sort of rotating wave around the bead. Have a pic somewhere, give me a minute to find.
[That's probably the worst description you'll read today!]
Here you go
(http://farm6.static.flickr.com/5057/5543190241_8b8d5678b1.jpg) (http://www.flickr.com/photos/blueboxstudio/5543190241/)
DSCN2348 (http://www.flickr.com/photos/blueboxstudio/5543190241/) by Blue Box Studio (http://www.flickr.com/people/blueboxstudio/), on Flickr
(http://farm6.static.flickr.com/5011/5543768856_c6932a1f34.jpg) (http://www.flickr.com/photos/blueboxstudio/5543768856/)
DSCN2187 (http://www.flickr.com/photos/blueboxstudio/5543768856/) by Blue Box Studio (http://www.flickr.com/people/blueboxstudio/), on Flickr
Oops, sorry, they are a bit big!!
I'd go for anything like these gravity beads ... or frits, enamels, etc ..... no two beads ever need to be the same, and if you keep a little pot of odd beads by your torch, you can select the right one to use as a size guide. If you aim for the same sized base bead before you add anything else, then you'll always end up with a set of nicely matched beads :)
Thank you, I haven't intentionally been making gravity beads it seems!!!
So pls induldge a thicko, make the disc thing, then add an outer of different coloured glass, melt it and let it sag into waves???
I've not tried to make those kind of gravity beads so can't advise I'm afraid, but you can use the same gravity process with frits to get effects like this too ...
(http://farm6.static.flickr.com/5217/5522548291_fe3f5d3b42.jpg) (http://www.flickr.com/photos/urbanbeads/5522548291/)
aDSCF2979 (http://www.flickr.com/photos/urbanbeads/5522548291/) by Mad Cat Glass (http://www.flickr.com/people/urbanbeads/), on Flickr
white base bead... roll in frit .... heat till it droops ... keep turning mandrel to stop it from blobbing on the table ... even up, pull out of flame and slowly balance the bead ... sorted ;)
I know I have to keep practicing, but I am a child of the instant gratification age and I want More an I want it NOW!!!!!!
No I'll keep at it. I will eventually get there I hope.
You have to take the positives, I no longer make brown sludge coloured beads regardless of the coloured glass I started with.
I have sorted out the sputnik spots, I am still struggling with dots as I find it like rubbing your head and patting your tummy or the other way around. The consequence of that is huge fat splodges which I end up raking, poking and changing.
I am proud I can make passable donut bead.
I don't get those murini things, I either blow them up or melt them so they resemble giant patterned splodges but not in a good way!!
I like coming here and drooling at all the fabulous work, the advice from everyone has been fantastic.
THANK YOU ALL!!!
Lyzeedee you sound very similar to me. that is where I am at. I can make beads of the right shape, and can now do that consistently so can make spacer type bracelets and necklaces, and etch them to give them some interest.
Then we get to the adding interest stage and I can do dots - sputnik like and they work.
Right now I am working on layered dots........... calling it my dotty period.......
However I think I may need another lesson soon as I am coming to a point where I would like guidance about what to practice then.
Done the gravity frit - they are great fun
Maybe I need to keep simple for a bit
Thanks and have fun
Sandra
twisted dots always looks good. also good to do where two colours join in general. very satisfying (and easy) to get that little spiral!
(this is where you plunge a cold stringer into a hot spot on your bead and twist)
also a good technique to do if your design has gone a bit....oopsie!
Thanks for posting this as it is where I am at too. I can make donuts and like doing dots, poked dots, layered dots and raised dots and now need to learn how to do other things. Sadly my job is keeping me very busy at the moment and I haven't had any time at the torch for a couple of weeks.
Well I have had an eureka moment thanks to this thread. I have made gravity beads and I am thrilled with them, five all the same combination of colours and roughly the same size, By George I've got it!!!!!
I have finally produced a few of the same and I am very happy.
I want to try the twirl thing with a stringer next and I hope one day to be able to make one of those lovely beach beads
Thank You
Hoorayy !! :)