Lampwork => Lampworking Tip n Tricks => Topic started by: Frenchie on March 18, 2011, 12:12:46 PM

Title: What's fuming?
Post by: Frenchie on March 18, 2011, 12:12:46 PM
I don't mean the jumpy up and down fuming... ;D  I think I read somewhere on here recently about how some glass fumes...?

What does this mean and what does it do...?  Is it a good thing..?

Title: Re: What's fuming?
Post by: Magpie on March 18, 2011, 12:48:34 PM
It's when the heavy metals like silver are heated and affect the glass you're working on. Either deliberately like was demoed at FO last year where you add a thin layer of silver or gold to your bead, or by mistake when you add a small dot of silver glass to your ivory bead and it goes all dark and yummy. It can be a good thing, but if it happens when you want a nice clear bead it can also be a bad thing. It's a bit like 'when does a flower become a weed'.

Someone will be along with the lady's name that did the demo and where her kits are etc soon as I can't remember, sorry.
Title: Re: What's fuming?
Post by: Pat from Canvey on March 18, 2011, 01:02:28 PM
Di East sells the kits, her website is http://www.glass2wear.com/
Title: Re: What's fuming?
Post by: Frenchie on March 22, 2011, 11:12:12 AM
aahh I see.  Get it now, thanks guys.
Title: Re: What's fuming?
Post by: RSimmons on August 23, 2011, 09:01:54 PM
One consideration is that fuming safely requires that you have excellent ventilation, otherwise you are putting potentially toxic heavy metal fumes into your immediate breathing area.

Robert
Title: Re: What's fuming?
Post by: Les on August 23, 2011, 09:36:41 PM
Oh believe me ... I've tried fuming without adequate ventillation ... it really does make you feel ill !